In this study, severe cracking occurred during an investigation of the direct hot rolling of industrial electrolytic nickel plates. To determine the cause of hot-rolling cracking, the microstructure phase composition was analyzed through the utilization of various techniques, including optical microscopy, scanning electron microscopy, electron backscattering diffraction, transmission electron microscopy (TEM), energy-dispersive X-ray spectroscopy (EDS) and electron probe micro-analysis. The comparative microstructural analysis took place between specimens heat treated in atmospheric and vacuum environments. The characterization and analysis of the hot-rolled plates considered the crack microstructure and fracture morphology. It was shown that holes appeared along the large angular grain boundaries after annealing at 1100 °C for 8 h. Possible reason: In a high-temperature environment, the decomposition of residual additives in the electrolytic nickel releases oxidizing gases, which oxidizes the grain boundaries. The reaction with carbon diffused into the grain boundaries and produced carbon monoxide gas, which induced holes and severely reduced the grain boundary plasticity. The heat treatment time did not need to be very long for severe grain boundary degradation to occur. After severe cavitation, the electrolytic nickel was severely cracked at grain boundaries cracks due to a shear force, and brittle fractures occurred along grains with very low plasticity.
Due to the characteristics of high salt and high acidity of the electrolyte and the chemical reaction between thiourea (Tu) and metal ions, it is still a problem to quickly and accurately detect Tu concentration in copper electrolyte. An improved spectrophotometric method has been proposed by simplifying the extraction steps of the traditional extraction–spectrophotometry and reducing the dosage of extractant and buffer. The improved method, with a favorable R2 of 0.9991, great precision of 1.67% and excellent spiked recovery of 102.19%, was not affected by the presence of gelatin and copper ions. Moreover, based on the spectrophotometry, a colorimetric method for rapid detection of Tu concentration in copper electrolyte was proposed. Using the standard color card produced enabled the expeditious determination of the concentration range of Tu in copper electrolyte. Since the gray value of the standard color card is linearly related to the Tu concentration, it is feasible to determine the Tu concentration by measuring the gray value of the test strip, and its accuracy was verified by spectrophotometry. The colorimetric method has satisfactory results in industrial practice. This study provides a novel approach for the rapid detection of Tu concentration in the copper electrolysis industry.
This study investigates the effect of different concentrations of lanthanum chloride (LaCl3) on the grain refinement of cobalt deposition layers during the electrochemical deposition process in industrial electrolytes. The impact of different LaCl3 concentrations on cobalt electrodeposition behavior was analyzed using the Liner sweep voltammetry curve (LSV), Cyclic voltammetry curve (CV), and Chronoamperometry curve (CA). The microstructure morphology and grain size of the deposition layers were analyzed using scanning electron microscopy and atomic force microscopy and the preferred orientation and crystal structure were analyzed using X-ray diffraction. The results show that the addition of different concentrations of LaCl3 to the industrial electrolyte leads to a negative shift in the starting deposition potential of cobalt, an increase in cathode polarization degree, an increase in overpotential, a shortened nucleation relaxation time tm and an accelerated nucleation rate during cobalt electrodeposition, resulting in grain refinement of the deposition layers. However, the addition of LaCl3 does not change the cobalt electrocrystallization mechanism, nor does it alter the crystal structure of the cobalt deposition layers, which remain in a close-packed hexagonal structure (HCP). When 0.2 g/L LaCl3 is added, the grain growth orientation changes from the (11\(\stackrel{\text{-}}{\text{2}}\)0) plane to the (11\(\stackrel{\text{-}}{\text{2}}\)0) and (10\(\stackrel{\text{-}}{\text{1}}\)0) planes, resulting in a uniform distribution of grain size and obvious grain refinement of the deposition layers.
12 December 2025 in Korean Journal of Chemical Engineering