Nickel- and zinc-doped TiO2(B) nanobelts were synthesized using a hydrothermal technique. It was found that the incorporation of 5 at.% Ni into bronze TiO2 expanded the unit cell by 4%. Furthermore, Ni dopant induced the 3d energy levels within TiO2(B) band structure and oxygen defects, narrowing the band gap from 3.28 eV (undoped) to 2.70 eV. Oppositely, Zn entered restrictedly into TiO2(B), but nonetheless, improves its electronic properties (Eg is narrowed to 3.21 eV). The conductivity of nickel- (2.24 × 10−8 S·cm−1) and zinc-containing (3.29 × 10−9 S·cm−1) TiO2(B) exceeds that of unmodified TiO2(B) (1.05 × 10−10 S·cm−1). When tested for electrochemical storage, nickel-doped mesoporous TiO2(B) nanobelts exhibited improved electrochemical performance. For lithium batteries, a reversible capacity of 173 mAh·g−1 was reached after 100 cycles at the current load of 50 mA·g−1, whereas, for unmodified and Zn-doped samples, around 140 and 151 mAh·g−1 was obtained. Moreover, Ni doping enhanced the rate capability of TiO2(B) nanobelts (104 mAh·g−1 at a current density of 1.8 A·g−1). In terms of sodium storage, nickel-doped TiO2(B) nanobelts exhibited improved cycling with a stabilized reversible capacity of 97 mAh·g−1 over 50 cycles at the current load of 35 mA·g−1.
Nanocrystalline layer-structured monoclinic Na2Ti3O7 is currently under consideration for usage in solid state electrolyte applications or electrochemical devices, including sodium-ion batteries, fuel cells, and sensors. Herein, a facile one-pot hydrothermal synthetic procedure is developed to prepare self-assembled moss-like hierarchical porous structure constructed by ultrathin Na2Ti3O7 nanotubes with an outer diameter of 6–9 nm, a wall thickness of 2–3 nm, and a length of several hundred nanometers. The phase and chemical transformations, optoelectronic, conductive, and electrochemical properties of as-prepared hierarchically-organized Na2Ti3O7 nanotubes have been studied. It is established that the obtained substance possesses an electrical conductivity of 3.34 × 10−4 S/cm at room temperature allowing faster motion of charge carriers. Besides, the unique hierarchical Na2Ti3O7 architecture exhibits promising cycling and rate performance as an anode material for sodium-ion batteries. In particular, after 50 charge/discharge cycles at the current loads of 50, 150, 350, and 800 mA/g, the reversible capacities of about 145, 120, 100, and 80 mA∙h/g, respectively, were achieved. Upon prolonged cycling at 350 mA/g, the capacity of approximately 95 mA∙h/g at the 200th cycle was observed with a Coulombic efficiency of almost 100% showing the retention as high as 95.0% initial storage. At last, it is found that residual water in the un-annealed nanotubular Na2Ti3O7 affects its electrochemical properties.
Neodymium doped yttrium aluminum garnet 4 at% Nd3+:Y3Al5O12 transparent ceramic was first fabricated by reactive spark plasma sintering using commercially available α-Al2O3, Y2O3, Nd2O3 powders as starting materials. Optimized sintering conditions were included two-steps: 1000 °C/3 min/100 °C min−1 and 1350 °C/5 min/30 °C min−1. 4 at% Nd3+:Y3Al5O12 ceramic had a homogenous microstructure with average grain size of 710 nm, and exhibited over 75 % transmittance in the visible wavelength range.