We successfully prepared butyl rubber (IIR)/polypropylene (PP) thermoplastic vulcanizate (IIR/PP-TPV) for shock-absorption devices by dynamic vulcanization (DV) using octyl-phenolic resin as a vulcanizing agent and studied the morphological evolution and properties during DV. We found that the damping temperature region of the IIR/PP-TPV broadened with the disappearance of the glass transition temperature (Tg) in the PP phase, which is ascribed to the improvement of compatibility between the IIR and PP with increasing DV time. As DV progresses, the size of the dispersed IIR particles and the PP crystalline phase decreases, leading to the formation of a sea–island morphology. After four cycles of recycling, the retention rates of tensile strength and elongation at break of the IIR/PP-TPV reached 88% and 86%, respectively. The size of the IIR cross-linking particles in the IIR/PP-TPV becomes larger after melt recombination, and the continuous PP phase provides excellent recyclability. Significantly, the prepared IIR/PP-TPV exhibits excellent recyclability, high elasticity, and good damping property.
22 November 2021 in Journal of Polymer Engineering
In order to obtain higher thermoelectric and mechanical properties in nonpolar thermoplastic vulcanizates (TPVs), the butyl rubber/polypropylene (TPVs)/hydroxylated graphene (HGE) composites with nanosheet network were prepared through masterbatch technique and based on thermodynamic calculations, using polypropylene-graft-maleic anhydride (PP-MA) as a compatibilizer. The Fourier transform infrared (FTIR) and Raman spectra revealed the introduced maleic anhydride group on PP-MA can form strong interfacial interaction with hydroxyl-containing functional groups on HGE. Morphology study indicated the rubber particles in the composites occupied the most volume of the PP phase, as expected to hinder the aggregation of HGE and form the effective nanosheet network. The nanosheet network can be combined with the butyl rubber (IIR) cross-linked particles during the dynamic vulcanization process to improve the interface bonding between PP and IIR, thus increasing the tensile strength of TPVs. The prepared TPVs/HGE composites have significantly improved in mechanical properties, thermal properties and dielectric properties, which provides a guarantee for their potential application as multifunctional TPVs polymers.
To achieve higher thermal electric and mechical properties in non-polar thermoplastic vulcanizate (TPV), multi-walled carbon nanotubes (MWCNTs) as reinforcing nanofiller to prepare TPV/MWCNTs conductive elastomer composites by dynamic vulcanization. The thermodynamic calculation indicates that MWCNTs have a tendency to preferentially localize at the two-phase interface of PP and IIR during melt-blending processing. The morphology of TPV/MWCNTs composites elucidated from TEM micrograph exhibited that the IIR domains dispersed in the PP matrix, and most MWCNTs were dispersed at the two-phase interface and PP phase, which is mainly due to the effect of kinetic factors. When the MWCNTs content reached the percolation threshold (3 wt%), the network structure of MWCNTs was formed, the ac conductivity and dielectric permittivity increased sharply. Compared with pristine TPV, the thermal conductivity of TPV/MWCNTs composites increased 39.7 %. The MWCNTs can combine to the IIR network during dynamic vulcanization, and enhances the interface interaction of MWCNTs and TPV matrix, which is improve the tensile strength of TPV/MWCNTs composites.