Microelectromechanical systems (MEMS) incorporating active piezoelectric layers offer integrated actuation, sensing, and transduction. The broad implementation of such active MEMS has long been constrained by the inability to integrate materials with giant piezoelectric response, such as Pb(Mg1/3Nb2/3)O3-PbTiO3 (PMN-PT). We synthesized high-quality PMN-PT epitaxial thin films on vicinal (001) Si wafers with the use of an epitaxial (001) SrTiO3 template layer with superior piezoelectric coefficients (e31,f = –27 ± 3 coulombs per square meter) and figures of merit for piezoelectric energy-harvesting systems. We have incorporated these heterostructures into microcantilevers that are actuated with extremely low drive voltage due to thin-film piezoelectric properties that rival bulk PMN-PT single crystals. These epitaxial heterostructures exhibit very large electromechanical coupling for ultrasound medical imaging, microfluidic control, mechanical sensing, and energy harvesting.
Chemical solution deposition (CSD) provides a low-cost, versatile approach for processing of thin and ultrathin ferroelectric films, as well as short and high aspect ratio ferroelectric nanostructures. This review discusses the state of the art in the processing of ferroelectric oxide thin films and nanostructures by CSD, with special emphasis on nucleation and growth phenomena. The effects of choice of precursor solution, substrate and bottom electrode stack, and thermal treatment conditions on the nucleation and growth are examined. Furthermore, methods to control ferroelectric thin film's microstructure, including phase content, texture, grain size and chemical homogeneity, are reviewed. Lastly, current CSD-based methods for processing of ferroelectric oxide nanostructures are presented with special consideration of the structural development, as well as advantages and shortcomings associated with each method. Lead zirconate-titanate, Pb(ZrxTi1−x)O3 (PZT), and barium titanate, BaTiO3 (BT), are used throughout the discussion, as specific examples for CSD processing of perovskite ferroelectrics.
A mechanism is described whereby 180° domain wall motion can contribute to the electrically induced strain in a ferroelectric material at subcoercive ac electric fields. The field-dependent, largely reversible motion of ferroelectric, 180° domain walls due to an applied ac electric field is considered. The Rayleigh law is modified to describe the piezoelectric response of the system. This results in both a linear dependence of the piezoelectric coefficient on the amplitude of the applied electric field and the creation of a second order harmonic of strain which adds to the electrostrictive response. The model was experimentally confirmed in thin films.
The extrinsic contributions to the dielectric response of thin films with (100) or (111) crystallographic orientation were studied (all indices are given in terms of the pseudocubic cell). Both the nonlinearity in the permittivity as well as the polarization hysteresis are described by the Rayleigh Law in subswitching conditions. It was found that (100) oriented films show a slightly higher extrinsic contribution to their dielectric behavior than (111) oriented films. For example, at 1 kHz and oscillation fields of , for (100) and (111) oriented films, respectively, 25% and 21% of the relative dielectric constant is due to irreversible extrinsic contributions. The difference is attributed to the higher concentration of mobile interfaces in the (100) oriented thin films. For frequencies between 20 Hz and 200 kHz both the Rayleigh parameters dropped with frequency approximately logarithmically. The frequency dependent Rayleigh parameters have been used to modify the Rayleigh Law to allow prediction of the dielectric properties in terms of both oscillation field and frequency.
Highly (100)-textured films (Lotgering factors ) with thicknesses ranging from 20 to 260 nm were grown on platinized Si substrates using sol-gel deposition. Ferroelectric hysteresis, low field dielectric permittivity, and nonlinear dielectric response as well as converse longitudinal piezoelectric response of the ultrathin films were studied at 1 kHz. The measurements revealed the existence of a critical film thickness, , below which the extrinsic contributions to the dielectric response are almost completely suppressed. Piezoelectric response of the films also showed a significant drop at the same critical thickness. Due to the columnar microstructure of these films the critical dimension of the ferroelectric is represented by the thickness rather than the lateral grain size, where the latter is invariant across the samples. The critical thickness led also to a deviation of the thickness dependence of the dielectric permittivity from the in-series capacitors model frequently representing “interfacial dead layers.” The critical size is attributed to significant reduction in domain wall population and/or mobility in films thinner than .