We report a significant enhancement in the electrical transport and photoconductivity of ZnO/ZnS core/shell nanowires (NWs) compared to those of ZnO NWs via the application of compressive strain. Under a compressive strain of −0.15%, the output current of the ZnO/ZnS core/shell NWs increases by 91.1% compared to that under the no-strain condition, whereas that of the ZnO NWs under the same condition is 42.7%. The significant increase in the output current of the ZnO/ZnS core/shell NWs is attributed to the type-II band alignment and strain-induced piezopotential changes at the junction interface, which induce a reduction in the barrier height to enable efficient charge carrier transport. Furthermore, under UV illumination and a compressive strain of −0.15%, although the photocurrent of the ZnO/ZnS core/shell NWs increases by 4.5 times compared to that of the ZnO NWs, the relative increase in the photocurrent of the ZnO/ZnS core/shell NWs is 11.7% compared to that under the no-strain condition, while the photocurrent of the ZnO NWs increases by 32.3% under the same condition. A decrease in the increase rate in the photocurrent of the ZnO/ZnS core/shell NWs with a change in strain under UV light compared to that under the dark condition can be explained by the piezoelectric screening effect induced by photogenerated carriers. By calculating the change in the Schottky barrier height (SBH), we demonstrate that the piezoelectric potential with a change in strain decreased the SBH, thus increasing the current level. Lastly, we propose a mechanism of the piezotronic and piezo-phototronic effects under applied strain and their effects on energy-band diagrams.
A previously unreported polymorph of 5,11-bis(triisopropylsilylethynyl)anthradithiophene (TIPS ADT), Form II, crystallizes from melt-processed TIPS ADT films blended with 16 +/- 1 wt % medium density polyethylene (PE). TIPS ADT/PE blends that initially are crystallized from the melt produce twisted TIPS ADT crystals of a metastable polymorph (Form IV, space group P1) with a brickwork packing motif distinct from the slipstack packing by solution-processed TIPS ADT crystals (Form I, space group P2(1)/c) at room temperature. When these films were cooled to room temperature and subsequently annealed at 100 degrees C, near a PE melting temperature of 110 degrees C, Form II crystals nucleated and grew while consuming Form IV. The growth rate and orientations of Form II crystals were predetermined by the twisting pitch and growth direction of the original banded spherulites in the melt-processed films of the blends. Notably, the Form IV -> II transition was not observed during thermal annealing of neat TIPS ADT films without PE. The presence of the mobile PE phase during thermal annealing of TIPS ADT/PE blend films increases the diffusion rate of TIPS ADT molecules, and the rate of nucleation of Form II. Form IV crystals are more conductive but less emissive compared to Form II crystals.