Climate change has important implication for the ecological environment and human social activities. The Qinghai-Tibet Plateau is a sensitive area for climate change, and the lakes on the Qinghai-Tibet Plateau are known as the “guardians” of climate change. However, there are few studies on the impact of climate variations on the exploitation of lithium resources in salt lakes. In this work, the collected data from Zabuye Salt Lake Observation Station and the experimental data of brine at different temperatures were employed as the research objects to investigate the relationship between regional climate change and lithium resources in salt lakes. The results indicated that Zabuye Salt Lake had abundant solar energy resources from 1991 to 2020 with the annual average sunshine duration of 3,122.4 h, the average annual evaporation of 2,579.07 mm/yr, and the annual average precipitation of 168.65 mm/yr. The average annual evaporation is around 15.3 times the average annual precipitation, owing to the short rainy season and the low rainfall. The phase diagram displayed that two lithium carbonate precipitation peaks clearly appeared at 25°C, and no obvious precipitation peak appeared at 15°C, indicating that a high-grade lithium carbonate mixed salt was prone to be formed at a higher temperature while lithium ions was more inclined to enrich in brine at a lower temperature. Therefore, Zabuye Salt Lake with the characteristics of low temperature, large temperature difference, less precipitation, strong radiation and large evaporation could be applied as unique lithium resources in the salt gradient solar pond, which would play a positive role in the development of salt lake resources.
Lithium, as the lightest alkali metal, is widely used in military and new energy applications. With the rapid growth in demand for lithium resources, it has become necessary to improve the effectiveness of extraction thereof. By using chemical grafting and electrospinning techniques, nanofibres containing crown ether were developed for adsorbing Li(I) from the brine in salt lakes, so as to selectively adsorb Li(I) on the premise of retaining specific vacancies of epoxy groups in crown ether. In lithium-containing solution, the adsorbing materials can reach adsorption equilibrium within three hours, and the maximum adsorption capacity is 4.8 mg g−1. The adsorption mechanisms of the adsorbing materials for Li(I) were revealed by combining Fourier transform infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), and X-ray photoelectron spectroscopy (XPS) with density functional theory (DFT) calculation. The results indicated that in crown ether, O in epoxy groups was coordinated with Li(I) to form Li–O and four O atoms in the epoxy groups were used as electron donors. After coordination, two O atoms protruded from the plane and formed a tetrahedral structure with Li(I), realising the specific capture of Li(I). By desorbing fibres that adsorbed Li(I) with 0.5-M HCl, the adsorption capacity only decreased by 10.4% after five cycles, proving ability to regenerate such materials. The nanofibres containing crown ether synthesised by chemical grafting and electrospinning have the potential to be used in extracting lithium resources from the brine in salt lakes.
Lithium is a key strategic metal in the 21st century and an important raw material in the new energy sector. With rapid growth of the market demand for lithium, the high-efficient extraction of lithium resources is of important economic significance. Taking zeolite as the carrier and using chemical grafting and electrospinning technologies, a kind of nanofiber containing crown ether (CE) was synthesized to adsorb Li(I) from the salt lake brine. This realizes the selective adsorption of Li(I) while retaining specific vacancies of epoxy groups in CE. The adsorption mechanism of nanofibers containing zeolite carriers and CE for Li(I) was revealed by the use of Fourier transform infrared (FT-IR) spectrometry, scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS), and density functional theory (DFT). The results show that after dsp3 hybridization of the outer orbit (2s) of Li(I), outer electrons on the nanofibers containing zeolite carriers and CE mainly migrate to the orbit for coordination with Li(I) thereat, thus realizing the capture of Li(I). The novel adsorbing material can reach adsorption equilibrium within 2.5 h and the adsorption kinetics for Li(I) conforms to the pseudo-second-order model and a maximum adsorption capacity of 8.6 mg/g. It can be found that the correlation coefficient fitted by Langmuir adsorption isotherm model is closer to 1, and the calculated maximum adsorption capacity is closer to the adsorption capacity obtained experimentally, therefore, it can be concluded that the adsorption process is more consistent with the Langmuir adsorption isotherm model, and the adsorption process can be regarded as monolayer adsorption. The adsorption capacity remains at 7.8 mg/g after 5 adsorption–desorption cycles, showing favorable stability and a strong ability to be regenerated. The research provides insights into the adsorption and recovery of Li(I) from the salt lake brine.