Husaini Ardy

Prof. Dr. Husaini Ardy

orcid

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
24 November 2020 in RSC Advances
Verified
Journal Article
Open access
PDF file
AWArie Wibowo
Arie Wibowo
MMMaradhana Agung Marsudi
Maradhana Agung Marsudi
MAMuhamad Ikhlasul Amal
Muhamad Ikhlasul Amal
MAMuhammad Bagas Ananda
Muhammad Bagas Ananda
RSRuth Stephanie
Ruth Stephanie
LDLina Jaya Diguna
Lina Jaya Diguna
Zinc oxide (ZnO) has been considered as one of the potential materials in solar cell applications, owing to its relatively high conductivity, electron mobility, stability against photo-corrosion and availability at low-cost.

2 April 2021 in Molecules
Verified
Journal Article
Open access
PDF file
AWArie Wibowo
Arie Wibowo
GTGusti U. N. Tajalla
Gusti U. N. Tajalla
MMMaradhana Agung Marsudi
Maradhana Agung Marsudi
Glen CooperGlen Cooper
Glen Cooper
LALia Asri
Lia Asri
Paulo BartoloPaulo Bartolo
Paulo Bartolo
Electroactive biomaterials are fascinating for tissue engineering applications because of their ability to deliver electrical stimulation directly to cells, tissue, and organs. One particularly attractive conductive filler for electroactive biomaterials is silver nanoparticles (AgNPs) because of their high conductivity, antibacterial activity, and ability to promote bone healing. However, production of AgNPs involves a toxic reducing agent which would inhibit biological scaffold performance. This work explores facile and green synthesis of AgNPs using extract of Cilembu sweet potato and studies the effect of baking and precursor concentrations (1, 10 and 100 mM) on AgNPs’ properties. Transmission electron microscope (TEM) results revealed that the smallest particle size of AgNPs (9.95 ± 3.69 nm) with nodular morphology was obtained by utilization of baked extract and ten mM AgNO3. Polycaprolactone (PCL)/AgNPs scaffolds exhibited several enhancements compared to PCL scaffolds. Compressive strength was six times greater (3.88 ± 0.42 MPa), more hydrophilic (contact angle of 76.8 ± 1.7°), conductive (2.3 ± 0.5 × 10−3 S/cm) and exhibited anti-bacterial properties against Staphylococcus aureus ATCC3658 (99.5% reduction of surviving bacteria). Despite the promising results, further investigation on biological assessment is required to obtain comprehensive study of this scaffold. This green synthesis approach together with the use of 3D printing opens a new route to manufacture AgNPs-based electroactive with improved anti-bacterial properties without utilization of any toxic organic solvents.

1 February 2021 in Heliyon
Verified
Journal Article
Open access
HAHusaini Ardy
Husaini Ardy
YPYudhistira Perdana Putra
Yudhistira Perdana Putra
AAAdimas Dwi Anggoro
Adimas Dwi Anggoro
AWArie Wibowo
Arie Wibowo
The primary Waste Heat Boiler (WHB) in an ammonia plant experienced cap leaking and the outer tube rupture after ten months since the last repair and replacement (total retubing). The leaking cap and the outer tube materials are low carbon steel SA-204 Gr. B and SA-209 Gr. T1a. The inappropriate vertical part of the leaked cap, which is 2.4 mm shorter than the design, might trigger turbulence flow inside the cap and lead to flow-accelerated corrosion (FAC), as suggested by the appearance of wall thinning and horseshoe pattern in the inner surface. This condition is severed by improper cap material selection with low chromium content (0.01%), which is more susceptible to FAC. The local turbulence flow might erode the oxide layer at the cap bottom and accumulate the oxide deposit around the circumference weld joint and the nearest nail spacer in the tube, represented by a thick Fe3O4 deposit. The primary WHB outer tube failure might occur due to the lack of cooling from boiler water because of cap leakage combined with a thick Fe3O4 scale deposit on the nail spacer that causes significant local temperature increases on the failed tube, which resulted in yielding and thin-lip rupture.

1 August 2019 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
HAHusaini Ardy
Husaini Ardy
DBDeri Andika Bangun
Deri Andika Bangun
Superheater tubes SA213 T12 (OD = 57 mm, WT = 6 mm) has been in service for 11 years in a supercritical coal fired boiler (315 MW). Tubes operating temperature are 430°C and pressure is 11 MPa. Failure occurred on tube no. 20, row 2. Three tubes specimens from the same row (failed tube, tube no. 3, and no. 4), were drawn for laboratory examinations. Vickers microhardnesses of failed and no. 3 tubes are the same (140 VHN), while tube no. 4 hardness is 170 VHN. These hardness values are much lower compared to the new tube (192 VHN). The lower hardness value of failed tube is due to complete decomposition of pearlite colonies in inner and outer side of failed tube to ferrite and spheroidized cementite. Failure of tube is characterized by thin lip rupture which indicated that the tube circumferential deformation occur gradually following spheroidization process. Failure by intergranular crack occurred along grain bondaries when the stress on the tube wall (hoop stress) exceeding material strength at service temperature. Tube no. 3 and 4 are partially spheroidized, mostly on the innerside. The severity of microstructure damage is related to the flow direction of flue gas, from tube no. 1 to no.2, no.3 and so on. Tube no. 1 was survived because it was protected by a front cover that will limit heat transfer from the flue gas. The previous failure analysis of similar boiler tube revealed that the hardness of the bulging tube is about 140 VHN which is the same as the hardness of the failed tube (no. 2) and no.3. Tube no. 3 is in the early stage of damage and shall be replaced because the hardness is much lower than 170 VHN. The effect of flue gas flow direction not only affects the hardness and microstructure but also deposit thickness. Deposit thickness in tube no. 2, 3, and 4 are 149, 123, and 100 µm respectively. Thicker deposit in tube no. 2 is also contributed to premature failure of this tube compared to the others. The local temperature of tube wall will be higher because thick deposit will reduce heat transfer between flue gas and steam inside the tube.

26 February 2023 in Heliyon
Verified
Journal Article
Open access
DADominico M. Aditya
Dominico M. Aditya
HAHusaini Ardy
Husaini Ardy
YLYorina S.F. Lantang
Yorina S.F. Lantang
YAYuli S. Afrianti
Yuli S. Afrianti
NINisa F.F. Ilmi
Nisa F.F. Ilmi
UPUdjianna S. Pasaribu
Udjianna S. Pasaribu
Cast austenitic stainless steel (CASS) has been widely used for long-term service periods in high-temperature applications. Nonetheless, the behavior of CASS after high-temperature and long-term service is insufficiently researched alongside the microstructural analysis for sigma phase and carbide. Here, intermediate pipe support made from CASS grade HH was investigated after 24 years of service at 700 °C and compared with the solution-treated specimen at 1100 °C for 2 h. The chemical composition was analyzed by optical emission spectroscopy (OES), while the microstructure was observed using optical microscopy and scanning electron microscope (SEM). The confirmation of phase composition and lattice parameters were further analyzed by energy-dispersive X-ray spectroscopy (EDS) and X-ray diffraction spectroscopy (XRD). The mechanical properties were assessed by tensile tests, hardness tests, and impact tests, whereas the corrosion property was analyzed using potentiodynamic polarization. Based on experiment and analysis, the effects of 24 years of exposure on the sigma phase are spheroidization and Cr depletion, and even partial transformation to ferrite. The sigma phase significantly increases the hardness, but Cr depletion slightly reduces the hardness to 96.86 HRB. Meanwhile, the carbide will increase in quantity and develop an irregular interface at long-term high-temperature exposure. Microstructure evolution of the sigma phase and carbide decreased tensile strength to 46%, elongation to 3%, and impact value to 1.6% of the minimum specifications, respectively, while the corrosion rate increased 10 times (about 7.35 μm per year).

3 May 2019 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
AWArie Wibowo
Arie Wibowo
ASAntonio R S A Sihombing
Antonio R S A Sihombing
APAde Wahyu Yusariarta Putra Parmita
Ade Wahyu Yusariarta Putra Parmita
UTUntung Triadhi
Untung Triadhi
HAHusaini Ardy
Husaini Ardy
Utilization of commercial Bacterial Celluloses (BCs) as catalyst support for preparation of heterogeneous fenton catalysts is attractive because catalytic activity of fenton catalyst can be increased by reducing their particles size. In this report, fenton catalyst@BC were prepared by sol gel method with fixed precursor concentration (0.5 M) and varied concentration of H2O2 (0.3, 0.6, 1.2 and 1.7 %v/v) to obtain optimum condition for fast degradation of Methylene Blue (MB). Scanning Electron Microscope (SEM) showed that micron-sized particles with particle sizes 1002.7 ± 511.5 nm has been successfully deposited on the surface of BC aerogel. Energy Dispersive Spectroscopy (EDS) results revealed that a small portion of iron oxide is observed in sample, even though the dominant elements in sample are sodium and chloride. UV-Vis spectroscopy unveiled that catalytic degradation profile of MB follows pseudofirst order reaction kinetics and the fastest degradation of MB was observed at 1.2 %v/v of H2O2 with Constanta of degradation rate (k) value is 2.65 × 10−2 min−1. Finding optimum condition for fastest degradation of MB is essential for the effort to completely remove dyes from clean water.