Improved methods to assess the degradation of coil coatings to approximate lifetime have been an area of academic and industrial interest for decades. This work aims to elucidate the differences in the degradation behavior of two coil coating systems: one standard commercial formulation and one formulation with a significant addition of biorenewable reactive diluents. Depth-resolved degradation behavior of samples exposed to accelerated and natural field weathering is assessed. Focal plane array attenuated total reflection-Fourier transform infrared spectroscopy was used to acquire high-resolution chemical data from a sloping cross section. The results agreed with conventional photoacoustic spectroscopy. Degradation profiles for the two coatings were significantly different, with the biobased samples showing a more durable behavior. This study provides a method for detailed assessment of coating degradation, giving a good estimation of its durability. This is both a way to compare the performance of coating systems and to improve the understanding of the impact of exposure conditions, paving the way for the development of more sustainable coil coatings.
11 April 2020 in Corrosion Engineering, Science and Technology: The International Journal of Corrosion Processes and Corrosion Control
Hot-dipped galvanised (HDG) steel and Zn5Al-coated steel were exposed for 6 years at different atmospheric weathering sites worldwide. The mass loss of the coatings has been measured after 1, 2, 4 and 6 years of exposure. In addition, corrosion products have been determined using scanning electron microscopy, X-ray diffraction and FTIR spectroscopy. It is shown that Zn5Al is better than HDG-steel independently on the exposure duration and location. The mass loss of Zn5Al is also less dependent of the environmental parameters (such as chloride deposition, relative humidity and temperature) than HDG-steel. The ratio of performance after 6 years of exposure varied from 1.3 to 5.1 with the mean value of 3.1. The analyses of the corrosion products indicate the formation of protective Zn/Al - layered double hydroxide (LDH) and sulphate-containing corrosion products of Zn and Al after 6 years of exposure. A mechanism explaining the superior properties of Zn5Al is proposed.
The initial atmospheric corrosion of ZM (ZnAlMg)-coated steel in humid air (85% RH) and humid argon (85% RH) containing 320 ppb SO2 was studied using in situ infrared reflection absorption spectroscopy (IRRAS), FTIR-ATR focal plane array (FPA) imaging and SEM-EDS. The corrosion products formed in humid air containing SO2 are mainly composed of magnesium sulphites and sulphates, with sulphite-containing corrosion products formed initially while the contribution from sulphates increased with exposure time. The results from FTIR-FPA imaging and SEM-EDS showed that the magnesium sulphite and sulphate are formed mainly on eutectic phases with a higher quantity of corrosion products formed on the binary eutectic (Zn-MgZn2) phases. This is due to presence of microgalvanic elements with the zinc-rich phases as the main sites for the cathodic oxygen reduction while the anodic reactions take place on the eutectic areas. Sulphate content is the highest on the binary eutectic phases, due to the microgalvanic effects and the production of oxidants by the cathodic reaction, which increases the oxidation of sulphite to sulphate.