Photocatalytic degradation is one of the effective methods to remove various pollutants from domestic and industrial effluents. Several operational parameters can affect the efficiency of photocatalytic degradation. Performing experimental methods to obtain the percentage degradation (%degradation) of pollutants in different operating conditions is costly and time-consuming. For this reason, the use of computational models is very useful to present the %degradation in various operating conditions. In our previous work, Fe 3 O 4 /TiO 2 nanocomposite containing different amounts of silver nanoparticles (Fe 3 O 4 /TiO 2 /Ag) were synthesized, characterized by various analytical techniques and applied to degradation of 2,4-dichlorophenol (2,4-DCP). In this work, a series of models, including stochastic gradient boosting (SGB), artificial neural network (ANN), adaptive neuro-fuzzy inference system (ANFIS), the improvement of ANFIS with genetic algorithm (GA-ANFIS), and particle swarm optimization (PSO-ANFIS) were developed to estimate the removal percentage of 2,4-DCP. The model inputs comprised of catalyst dosage, radiation time, initial concentration of 2,4-DCP, and various volumes of AgNO 3 . Evaluating the developed models showed that all models can predict the occurring phenomena with good compatibility, but the PSO-ANFIS and the SGB models gave a high accuracy with the coefficient of determination ( R2 ) of 0.99. Moreover, the relative contributions, and the relevancy factors of input parameters were evaluated. The catalyst dosage and radiation time had the highest (32.6%), and the lowest (16%) relative contributions on the predicting of removal percentage of 2,4-DCP, respectively.
Titanium-pillared clay (Ti-PILC), as one of the most suitable types of porous adsorbents/(photo)catalysts, was prepared from a local type of Iranian clay and titanium isopropoxide. The production process was optimized by changing three operating parameters, including the clay suspension concentration (in the range of 0.5–10% w/v), the H+/Ti ratio (2–8 mol/mol), and the calcination temperature (300–700 °C). The largest specific surface area for the Ti-PILC was about 164 m2/g under the clay suspension of 0.5% w/v, H+/Ti = 6, with a surface area 273% larger than that of the raw clay. The surface areas obtained from more concentrated clay suspensions were, however, comparable (159 m2/g for 3% w/v clay and H+/Ti = 4). An increase in the calcination temperature has a negative effect on the porous texture of Ti-PILC, but based on modeling with artificial neural networks, its contribution was only 7%. Clay suspension and H+/Ti ratio play a role of 56 and 37% of the specific surface area. The presence of rutile phase, and in some cases anatase phase of TiO2 crystals was detected. FTIR and SEM investigations of Ti-PILCs produced under different operating parameters were analyzed.