In this paper, the concept of incorporating core–shell structured units as secondary phases to toughen Al2O3 ceramics is proposed. An Al2O3 composite ceramic toughened by B4C@TiB2 core–shell units is successfully synthesized using a combination of molten salt methodology and spark plasma sintering. The synthesis of B4C@TiB2 core–shell toughening units stems from the prior production of core–shell structural B4C@TiB2 powders, and this core–shell structure is effectively preserved within the Al2O3 matrix after sintering. The B4C@TiB2 core–shell toughening unit consists of a micron-sized B4C core enclosed by a shell approximately 500 nm thick, composed of numerous nanosized TiB2 grains. The regions surrounding these core–shell units exhibit distinct geometric structures and encompass multidimensional variations in phase composition, grain dimensions, and thermal expansion coefficients. Consequently, intricate stress distributions emerge, fostering the propagation of cracks in multiple dimensions. This behavior consumes a considerable amount of crack propagation energy, thereby enhancing the fracture toughness of the Al2O3 matrix. The resulting Al2O3 composite ceramics displays a relative density of 99.7±0.2%, a Vickers hardness of 21.5±0.8 GPa, and a fracture toughness 6.92±0.22 MPa·m1/2.
In this study, we propose a novel approach to enhance the fracture toughness of Al2O3 ceramics by incorporating core-shell structural composite whiskers as secondary phases. In particular, Al2O3 composite ceramics reinforced with TiC-coated SiC whiskers (SiCw@TiC) were successfully fabricated through a combination of molten salt synthesis and spark plasma sintering. The SiCw@TiC whiskers feature a SiCw core and a TiC shell layer (~85 nm thick) composed of nano-sized TiC grains. Remarkably, the core-shell structure is preserved within the Al2O3 matrix after sintering, forming a unique composite toughening phase. The interfacial regions surrounding the whiskers exhibit a complex geometric configuration and multi-dimensional heterogeneities, including variations in phase composition (Al2O3/SiC/TiC), grain size (micron/nano nanoscale), and thermal expansion coefficients (3.8-7.4×10-6/K), which collectively generate a sophisticated stress field. This intricate microstructure enables the SiCw@TiC whiskers to dissipate crack propagation energy through multiple mechanisms, significantly improving the fracture toughness of the Al2O3 matrix. The resulting Al2O3-SiCw@TiC composite ceramics demonstrate exceptional mechanical properties, with a relative density of 99.16 ± 0.48 %, Vickers hardness of 21.38 ± 0.93 GPa, flexural strength of 693 ± 49 MPa, and fracture toughness of 7.15 ± 0.47 MPa·m1/2. This work establishes a paradigm for structural ceramic toughening through engineered core-shell architectures.
Thermoplastic polyurethane (TPU) belongs to a polyurethane family that possesses an elongation much higher than 300%, despite having low mechanical strength, which can be overcome by incorporating clay-based halloysite nanotubes (HNTs) as additives to manufacture TPU/HNT nanocomposites. This paper focuses on the co-influence of HNT content and 3D printing parameters on the mechanical properties of 3D printed TPU/HNT nanocomposites in terms of tensile properties, hardness, and abrasion resistance via fused deposition modelling (FDM). The optimum factor-level combination for different responses was determined with the aid of robust statistical Taguchi design of experiments (DoEs). Material characterisation was also carried out to evaluate the surface morphology, nanofiller dispersion, chemical structure, thermal stability, and phase behaviour corresponding to the DoE results obtained. It is evidently shown that HNT level and infill density play a significant role in impacting mechanical properties of 3D-printed TPU/HNT nanocomposites.
1 February 2021 in Journal of the European Ceramic Society