Micro-alloyed Mg-0.4 (wt.%) La alloy is recommended for Mg-air battery anode material. Two Mg-La anodes with different microstructures, i.e., as-cast and extruded, are fabricated by casting and extrusion technology. The effect of morphologies on discharge of Mg-La alloys is studied and examined by anodic self-discharge behavior and discharge performance. The extruded Mg-La anode releases less hydrogen during the discharge and shows limited chunk effect than the as-cast anode. Anodic efficiency is enhanced consequently, reaching 77.3% at 10 mA cm –2 . This alloy enhances the discharge property of Mg-air battery and enables cell with higher voltage and energy density, compared with the as-cast alloy and re-cast Mg.
AZ63 sacrificial anode is widely used to protect buried metal pipelines and reinforced concrete structures and so on. The interfacial metallurgical bonding between AZ63 sacrificial anode and Q235 wiring terminal directly affects its cathodic protection performance. Therefore, microstructure and mechanical properties of interfacial between AZ63 and Q235 by solid–liquid compound casting with hot-dip galvanized and post-casting solution-aging treatment (T6) were investigated. The results indicate that hot-dip galvanizing on the surface of Q235 is beneficial to the formation of intermetallic compounds at the interface. At the same time, it can promote the metallurgical bonding of the interface between AZ63 and Q235. After T6 heat treatment, the intermetallic compound at the interface between AZ63 and galvanized Q235 was refined. The electron-probe microanalyzer (EPMA) revealed that the intermetallic compounds at the interfaces between AZ63 and galvanized Q235 were Fe2Al5 before and after T6 treatment. Push-out testing and microhardness were used to investigate the mechanical properties of interface between AZ63 and Q235. It is shown that the hot-dip galvanization of the Q235 surface and T6 treatment were beneficial to improve the metallurgical bonding shear strength and microhardness of the interface. After T6 heat treatment, the highest shear strength at the interface between AZ63 and galvanized Q235 was up to 31.9 ± 1.9 MPa.