The early-stage M23C6 morphology at the phase boundary between austenite and δ ferrite grain in Type 304L austenitic stainless steel was investigated with transmission electron microscopy (TEM). The M23C6 has coherency with austenite grains at phase boundary. The phase boundary between the M23C6 and austenite grains has curved appearance. The curved phase boundary might be a faceted interface composed of (111) plane and the other low-index planes on the atomic scale. The M23C6 morphology at the phase boundary was identified to be a complex pyramid-like shape that has {111}, {110} and {100} interfaces. The slight deviation in the angle measured between edges of carbide in the TEM images from that calculated between edges expected from the M23C6 morphology might be attributed to multilayer growth in the interior region of the M23C6 face.
Abstract: Stress corrosion cracking (SCC) is one of major threats against the integrity of the structural materials composing a nuclear power plant (NPP). Lead is deleterious element accelerating the SCC of Alloy 600 used as a steam generator tubing material in an NPP. In the present work, the oxide property grown on an Alloy 600 surface was evaluated as a function of PbO content using electrochemical impedance spectroscopy (EIS) and a field-emission transmission electron microscopy, equipped with an energy dispersive X-ray spectroscopy (TEM –EDS) for the specimen prepared using a focused ion beam (FIB). Alloy 600 was immersed in 0.1M NaOH containing PbO in the range of 0-5,000 ppm at 315oC for 2 weeks. The oxide property was compared with SCC susceptibility obtained from a slow strain rate tension (SSRT) test for Alloy 600 in 0.1M NaOH containing PbO. The impedance value was greatly decreased by adding PbO into the solution indicating a decrease in passivity. The composition of the oxide was also changed by Pb in an aqueous solution. The duplex oxide layer consisting of outer porous nickel-rich oxide and inner dense chromium-rich oxide is modified to a Pb incorporated nickel-rich oxide layer. Modification of the oxide property induced by lead incorporation caused an obvious increase in SCC susceptibility. It is expected that lead observed at the crack tip of an early cracked pulled Alloy 600TT tube was considerably responsible for SCC acceleration of this tube among numerous sound tubes in an NPP.
1 June 2017 in Archives of Metallurgy and Materials
Effects of grain boundary morphologies on stress corrosion cracking (SCC) of Alloy 600 have been studied in 40% NaOH at 315°C using C-ring specimens. The configuration of the grain boundary and the intergranular carbide density were controlled by heat treatment. SCC tests were performed at +150 mV above the corrosion potential. The specimen with a serrated grain boundary showed higher SCC resistance than that with a straight grain boundary. This appears to be caused by the fact that the specimen with the serrated grain boundary has longer SCC path. SCC resistance also increased with intergranular carbide density probably due to enhanced relaxation of stress at intergranular carbide.
12 September 2013 in Journal of Solid State Electrochemistry