The configurational entropy is an emerging descriptor in the functional materials genome. In thermoelectric materials, the configurational entropy helps tune the delicate trade‐off between carrier mobility and lattice thermal conductivity, as well as the structural phase transition, if any. Taking GeTe as an example, low‐entropy GeTe generally have high carrier mobility and distinguished zT > 2, but the rhombohedral‐cubic phase transition restricts the applications. In contrast, despite cubic structure and ultralow lattice thermal conductivity, the degraded carrier mobility leads to a low zT in high‐entropy GeTe. Herein, medium‐entropy alloying is implemented to suppress the phase transition and achieve the cubic GeTe with ultralow lattice thermal conductivity yet decent carrier mobility. In addition, co‐alloying of (Mn, Pb, Sb, Cd) facilitates multivalence bands convergence and band flattening, thereby yielding good Seebeck coefficients and compensating for decreased carrier mobility. For the first time, a state‐of‐the‐art zT of 2.1 at 873 K and average zTave of 1.3 between 300 and 873 K are attained in cubic phased Ge0.63Mn0.15Pb0.1Sb0.06Cd0.06Te. Moreover, a record‐high Vickers hardness of 270 is attained. These results not only promote GeTe materials for practical applications, but also present a breakthrough in the burgeoning field of entropy engineering.
13 September 2020 in Advanced Functional Materials
Band convergence and optimization of carrier density play significant roles in enhancing thermoelectric figure of merit (ZT). In this study, using combined experimental and computational studies, we have systemically revealed the electronic origin of high-average ZT in Pb-doped GeTe-based alloys. The intrinsic high hole-carrier density of GeTe is firstly reduced to a rough optimal range by Bi doping, and then the carrier density is finely tuned by Pb doping. The band convergence by Pb doping can maintain the relatively high power factor of GeTe-based alloys when the carrier density is reduced by Pb doping. Moreover, further reduction of lattice thermal conductivity and fine tuning of carrier density by Pb doping can maximize the ZT at corresponding carrier density, therefore realizing high-average ZT. A peak ZT of ∼2.0 at 573 K and an average ZT of ∼1.50 within 300–773 K can be obtained in Ge0.96(1−x)Pb0.96xBi0.08Te1.08 with x = 0.15. This work demonstrates the great positive effects of Pb for high-average ZT in GeTe-based alloys, and also provides a guide for the rational use of Pb.
15 June 2020 in ACS Applied Materials & Interfaces