Linshan Wang

Dr. Linshan Wang


Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
1 March 2024 in Materials Research Express
Verified
Journal Article
Open access
PLPengcheng Lin
Pengcheng Lin
LWLinshan Wang
Linshan Wang
XLXuebing Liang
Xuebing Liang
QHQiang Hu
Qiang Hu
LWLimin Wang
Limin Wang
Xuanhui QuXuanhui Qu
Xuanhui Qu
Copper-infiltrated sintered steel is a prominent area of research in powder metallurgy, with a particular focus on enhancing impact toughness. In this study, sintered steels with varying pore structures were prepared using iron powders and infiltrated with copper to investigate their impact toughness. The results indicate a significant improvement in the impact toughness of the sintered steels with concentrated iron particle sizes. The density of the samples increased from 6.85 g cm−3 to 7.55 g cm−3 through copper infiltration. The large copper-phase sample with the particle size of 150 μm exhibits an impact toughness as high as 41.09 J cm−2, and its fracture morphology mainly shows transgranular fractures of large iron particles. It is 1.5 times that of the sample made from commercial iron powders which measured 27.46 J cm−2. This enhancement is primarily attributed to the precipitation of γ-Fe within the large copper phase, thereby enhancing the copper phase and transferring the load into large iron particles. A brief mechanism of γ-Fe precipitation in the large copper-phase has been provided.

5 June 2025 in Metals
Verified
Journal Article
Open access
PDF file
PLPengcheng Lin
Pengcheng Lin
LWLinshan Wang
Linshan Wang
SLShuanghua Liang
Shuanghua Liang
XLXuebing Liang
Xuebing Liang
QHQiang Hu
Qiang Hu
Xuanhui QuXuanhui Qu
Xuanhui Qu
This study employs CT non-destructive detection to quantitatively analyze the pore structure of sintered steel and investigate copper infiltration mechanisms. As density increases from 6.55 to 6.95 g/cm3, pore characteristics exhibit significant changes: pore quantity initially increases then decreases, while average pore size monotonically reduces from 35.7 to 17.2 μm. Copper infiltration dramatically transforms the material’s porosity, characterized by reduced pore count, decreased distribution uniformity, increased closed pore proportion, and morphological regularization. The infiltration process demonstrates selective filling, primarily governed by pore connectivity, size effect, and capillary forces. Molten copper preferentially penetrates high-connectivity networks, prioritizing irregular angular regions. Medium-sized pores (10.52–23.76 μm) with optimal connectivity are predominantly filled. At 6.75 g/cm3, an optimal balance between pore quantity, size, and connectivity facilitates uniform copper infiltration.

24 August 2022 in Materials
Verified
Journal Article
Open access
PDF file
FZFengshi Zheng
Fengshi Zheng
LWLinshan Wang
Linshan Wang
RWRui Wang
Rui Wang
WJWang Jianwei
Wang Jianwei
SZShaoming Zhang
Shaoming Zhang
LWLimin Wang
Limin Wang
We investigated the effect of different sintering temperatures ranging from 200 °C to 600 °C on the porous properties and pore microstructure of large capillary pressure wicks made of carbonyl nickel powder. The evolution model of hydraulic diameter was established and verified by the maximum pore diameter. Hydraulic diameter changed as the roughness of particle surfaces decreased and sintering necks grew large during sintering. In the contact-formation stage and the initial sintering stage (200–500 °C), the decrease in the roughness of particle surfaces played a decisive role, contributing to an increase in hydraulic diameter. In the intermediate sintering stage (600 °C), the growth of sintering necks dominated the process, however the hydraulic diameter was reduced. These results show that the maximum pore diameter first increased and then decreased in the same way as our evolution model. Permeability and capillary performance of the wicks first increased and then declined with increasing sintering temperature. We found the optimal sintering temperature to be 400 °C, at which point the wicks achieved the maximum pore diameter of 1.21 μm, a permeability of 1.77 × 10−14 m2, and their highest capillary performance of 1.46 × 10−8 m.

10 October 2022 in Metals
Verified
Journal Article
Open access
PDF file
FZFengshi Zheng
Fengshi Zheng
LWLinshan Wang
Linshan Wang
SZShaoming Zhang
Shaoming Zhang
LZLin Zhang
Lin Zhang
QHQiang Hu
Qiang Hu
LWLimin Wang
Limin Wang
This study prepared pre-sintered clusters with fine nickel powders and proposed an effective method to predict and control the sintering shrinkage based on cluster size. Experiments were conducted to investigate the influence of the pre-sintering temperature and cluster size on the specific surface area and morphology of pre-sintered clusters as well as to validate the availability of the proposed shrinkage prediction method. The results show that the specific surface area decreases with an increasing pre-sintering temperature and slightly oscillates with an increasing cluster size. The linear shrinkage ratio is inversely proportional to the cluster size and decreases with an increasing pre-sintering temperature, which begins to drop rapidly at 500 °C and decreases from 19.05% to 3.18% at 800 °C. The experimental results are quite approximate to the predicted values, which strongly prove the availability of the proposed shrinkage prediction method.

8 January 2025 in Advances in Engineering Technology Research
Verified
Journal Article
Open access
PDF file
SLShuanghua Liang
Shuanghua Liang
LWLinshan Wang
Linshan Wang
XLXuebing Liang
Xuebing Liang
FZFengshi Zheng
Fengshi Zheng
QHQiang Hu
Qiang Hu
With the rapid development of new energy vehicles and communication technologies, the demand for high-performance copper thermal conductive components is increasing. Manufacturing copper thermal conductive components with complex structures by metal injection molding is one of the most optimal solutions. In this paper, water-atomized copper powder with an average particle size of 29.75 µm is used as raw material, and the effect of spheroidization treatment on the properties of copper powder, such as morphology, particle size, apparent density, and tap density, is studied, as well as the effect on the metal injection molding. The results show that the properties of copper powder treated at 960 r/min were significantly improved compared with those of untreated copper powder, with the average particle size reduced by 27.4%, the sphericity increased by 7.6%, the surface roughness reduced by 30.7%, and the apparent density and tap density increased by 18.8% and 3.2%, respectively. The powder loading rate of the feedstock reached 60%, and the flow behavior index and flow activation energy of the feedstock were the lowest, with good rheological properties. The sintered densification of the sample reached 98.1%, which was 2.4% higher than that of the untreated copper powder.

26 December 2024 in Journal of Materials Engineering and Performance
Verified
Journal Article
Closed access
PDF file
PLPengcheng Lin
Pengcheng Lin
LWLinshan Wang
Linshan Wang
XLXuebing Liang
Xuebing Liang
QHQiang Hu
Qiang Hu
LWLimin Wang
Limin Wang
XQXuanhui Qu
Xuanhui Qu