In the present study, an icosahedral single phase bulk quasicrystalline material based on Al62Cu25.5Fe12.5 has been synthesised by a spray forming route. Microstructural characterization showed an average grain size of 10 μm. The oversprayed fine powder showed the presence of β- and λ-phases, whereas, the deposit consited of the fully single phase bulk quasicrystalline material with compositional homogeneity. The hardness and fracture toughness measurements were carried out at different indentation loads of 50–500 g. The hardness values varied in the range 10.4–8.1 GPa and fracture toughness was seen to decrease with increasing load. The varionan of hardness with load, which is known as indentation size effect (ISE), has been established clearly. Fracture toughness value was constant in the load range from 200 to 500 g at 1.2 MPa m1/2. The cracking pattern after indentation at higher load has been observed to be intergranular as well as transgranular. The evolution of the single phase bulk quasicrystalline material has been discussed in light of the unique combination of atomization and deposition process elements in spray forming technique.
In the present investigation, the indentation study on the high-energy ball-milled nanocrystalline Al5Fe2 intermetallic compound has established the inverse Hall–Petch (IHP) behaviour. The structural characterisation of the milled powder particles by X-ray diffraction (XRD) and transmission electron microscopy has shown the evolution of nanocrystalline phase. Micro-indentation measurements have revealed the increase in hardness with decreasing grain size, reaching to a maximum of 9.0 ± 0.3 GPa up to a grain size of 32 ± 4 nm, followed by a decrease. The decrease in hardness with further refinement, an indication of grain size softening, demonstrates the IHP-like behaviour. The deviation from the Hall–Petch behaviour has been discussed using various models based on the dislocations and grain boundary-mediated processes. From the analysis, it appears that the model based on mesocopic grain boundary sliding phenomena is more appropriate to account for the observed grain size softening.
3 December 2014 in Metallurgical and Materials Transactions A