Zhiyong Dai

Dr. Zhiyong Dai


Research Focus & Metrics

Academic Career Length

5Years (2022-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
28 August 2024 in Crystals
Verified
Journal Article
Open access
PDF file
YWYingdi Wang
Yingdi Wang
YSYunhai Su
Yunhai Su
ZDZhiyong Dai
Zhiyong Dai
Inconel 625 deposited metal was prepared by gas metal arc welding. The solid solution treatment temperature was set at 1140 °C for 4 h using the DSC test method, followed by secondary aging at 750 °C/4 h and 650 °C/24 h. The specimens in the prepared state and after heat treatment were subjected to high temperature tensile at 600 °C, respectively. The fracture morphology, thermal deformation behavior, and strengthening mechanism of the samples in different states were analyzed. The results showed that the stress–strain curves of the deposited metals exhibited obvious work-hardening behavior at 600 °C. The solid solution and aging heat-treated samples have higher tensile and yield strength, but the plasticity is obviously lower than that of the deposited metal. It was also found that the γ″ phase and M23C6 carbides, as well as the continuous stacking faults in the alloy, were the main reasons for the increase in tensile strength of the solution and aging heat-treated sample.

10 December 2022 in Materials
Verified
Journal Article
Open access
PDF file
TYTaisen Yang
Taisen Yang
YSYunhai Su
Yunhai Su
ZDZhiyong Dai
Zhiyong Dai
YWYingdi Wang
Yingdi Wang
XLXuewei Liang
Xuewei Liang
ZWZuyong Wei
Zuyong Wei
In this paper, the element nitrogen (N) is used to partially replace the element nickel (Ni) in flux-cored wire. A 44%Ni-24%Cr-0.18N nitrogen-containing low-nickel flux-cored wire with excellent corrosion resistance is prepared. The corrosion behavior of nitrogen-containing low-nickel weld cladding and Inconel 625 weld cladding in 40 KCl + 60 MgCl2 (wt%) molten salt at 900 °C is studied. The results show that the selective dissolution of Cr occurs in both weld claddings. The corrosion resistance of the 44%Ni-24%Cr-0.18N nitrogen-containing low-nickel weld cladding is better than that of the Inconel 625 weld cladding. The reason is that added N can react with H+ in molten salt to generate NH4+, remove corrosive impurities of MgOH+ in molten salt and change the corrosion environment. N preferentially combines with Cr to form Cr2N, reduces the diffusion precipitation of Cr and improves the corrosion resistance.

21 August 2023 in Journal of Materials Science
Verified
Journal Article
Closed access
PDF file
TYTaisen Yang
Taisen Yang
GZGuiqing Zhang
Guiqing Zhang
ZDZhiyong Dai
Zhiyong Dai
XLXuewei Liang
Xuewei Liang
YWYingdi Wang
Yingdi Wang
YSYunhai Su
Yunhai Su

30 October 2024 in Crystals
Verified
Journal Article
Open access
PDF file
YWYingdi Wang
Yingdi Wang
ZDZhiyong Dai
Zhiyong Dai
YSYunhai Su
Yunhai Su
Nitrogenous nickel-based deposited metal was prepared by using the gas metal arc welding (GMAW) method, and it was further subjected to solid-solution and aging heat treatment. The influence of different solid-solution temperatures on the microstructure of the deposited metal was studied, and the complete heat treatment system for the nitrogenous nickel-based deposited metal was ultimately determined. The microstructure, mechanical properties, and deformation mechanism of the nitrogenous nickel-based deposited metal in two states (as-prepared state and complete heat-treated state) were finally investigated. The results show that the microstructure of the deposited metal mainly consisted of epitaxially grown columnar grains with large grains. Petal-like Laves phases formed between the dendrites. The main deformation mechanism was the unit dislocation a/2 cut precipitation phase. After a complete heat treatment, all the Laves phases were re-melted, and nanoscale M(C,N) phases precipitated in the grains, while M23C6 phases formed at the grain boundaries. The samples showed higher yield and ultimate tensile strengths than those of the as-prepared state metal, but with reduced ductility. The deformation mechanism involved not only a/2 matrix dislocations cutting the precipitated phase, but also two a/6 Shockley incomplete dislocations, together cutting the precipitated phase to form a stacking layer dislocation.