James Aluha

Dr. James Aluha


Research Focus & Metrics

Academic Career Length

10Years (2017-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
12 October 2018 in Nanomaterials
Verified
Journal Article
Open access
PDF file
JAJames Aluha
James Aluha
SGStéphane Gutierrez
Stéphane Gutierrez
FGFrancois Gitzhofer
Francois Gitzhofer
Nicolas AbatzoglouNicolas Abatzoglou
Nicolas Abatzoglou
A study was done on the effect of temperature and catalyst pre-treatment on CO hydrogenation over plasma-synthesized catalysts during the Fischer–Tropsch synthesis (FTS). Nanometric Co/C, Fe/C, and 50%Co-50%Fe/C catalysts with BET specific surface area of ~80 m2 g–1 were tested at a 2 MPa pressure and a gas hourly space velocity (GHSV) of 2000 cm3 h−1 g−1 of a catalyst (at STP) in hydrogen-rich FTS feed gas (H2:CO = 2.2). After pre-treatment in both H2 and CO, transmission electron microscopy (TEM) showed that the used catalysts shifted from a mono-modal particle-size distribution (mean ~11 nm) to a multi-modal distribution with a substantial increase in the smaller nanoparticles (~5 nm), which was statistically significant. Further characterization was conducted by scanning electron microscopy (SEM with EDX elemental mapping), X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). The average CO conversion at 500 K was 18% (Co/C), 17% (Fe/C), and 16% (Co-Fe/C); 46%, 37%, and 57% at 520 K; and 85%, 86% and 71% at 540 K respectively. The selectivity of Co/C for C5+ was ~98% with 8% gasoline, 61%, diesel and 28% wax (fractions) at 500 K; 22% gasoline, 50% diesel, and 19% wax at 520 K; and 24% gasoline, 34% diesel, and 11% wax at 540 K, besides CO2 and CH4 as by-products. Fe-containing catalysts manifested similar trends, with a poor conformity to the Anderson–Schulz–Flory (ASF) product distribution.

14 September 2020 in Materials
Verified
Journal Article
Open access
PDF file
FBFaranak Barandehfard
Faranak Barandehfard
JAJames Aluha
James Aluha
AHAlireza Hekmat
Alireza Hekmat
FGFrancois Gitzhofer
Francois Gitzhofer
The corrosion of refractories in contact with high temperature aluminum-magnesium alloys leads to contamination of the Al-Mg alloy products by solid impurities from degraded refractories. Where both the spinel and corundum phases form in the refractories, cracks are generated and propagated by diffusion of molten Al-Mg, resulting in severe corrosion. In this review paper, the corrosion phenomenon is discussed, and published work is summarized, supplemented by our recent experimental results. Using the Alcan immersion test, materials based on white-fused mullite (WFM) were evaluated for their corrosion resistance and interfacial behavior. WFM was modified using different 2-wt.% of non-wetting additives (NWAs), such as BaSO4, CaF2, Secar®71 cement and wollastonite to improve their performance when in contact with molten Al-Mg alloy at 850 °C for 96 h. The mechanical properties of the samples such as flexural and compressive strength were evaluated, in addition to X-ray diffraction and microscopic analysis (optical and scanning electron microscopy coupled with X-ray elemental mapping). It was observed that cracks formed in samples were promoted with only BaSO4, CaF2, Secar®71 cement or wollastonite. However, cracks did not appear in the sample promoted with both 1-wt.% CaF2 and 1-wt.% BaSO4, because of improved anti-wetting properties in addition to inhibiting spinel (MgAl2O4) formation, which is the main cause of the cracks. This is a significant finding in the prevention of cracks and improvement of the refractory corrosion resistance.

21 February 2017 in Catalysts
Verified
Journal Article
Open access
PDF file
JAJames Aluha
James Aluha
YHYongfeng Hu
Yongfeng Hu
Nicolas AbatzoglouNicolas Abatzoglou
Nicolas Abatzoglou
A plasma-synthesized cobalt catalyst supported on carbon (Co/C) was tested for Fischer-Tropsch synthesis (FTS) in a 3-phase continuously-stirred tank slurry reactor (3-φ-CSTSR) operated isothermally at 220 °C (493 K), and 2 MPa pressure. Initial syngas feed stream of H2:CO ratio = 2 with molar composition of 0.6 L/L (60 vol %) H2 and 0.3 L/L (30 vol %) CO, balanced in 0.1 L/L (10 vol %) Ar was used, flowing at hourly space velocity (GHSV) of 3600 cm3·h−1·g−1 of catalyst. Similarly, other syngas feed compositions of H2:CO ratio = 1.5 and 1.0 were used. Results showed ~40% CO conversion with early catalyst selectivity inclined towards formation of gasoline (C4–C12) and diesel (C13–C20) fractions. With prolonged time-on-stream (TOS), catalyst selectivity escalated towards the heavier molecular-weight fractions such as waxes (C21+). The catalyst’s α-value, which signifies the probability of the hydrocarbon chain growth was empirically determined to be in the range of 0.85–0.87 (at H2:CO ratio = 2), demonstrating prevalence of the hydrocarbon-chain propagation, with particular predisposition for wax production. The inhibiting CO effect towards FTS was noted at molar H2:CO ratio of 1.0 and 1.5, giving only ~10% and ~20% CO conversion respectively, although with a high α-value of 0.93 in both cases, which showed predominant production of the heavier molecular weight fractions.

23 April 2021 in Coatings
Verified
Journal Article
Open access
PDF file
FBFaranak Barandehfard
Faranak Barandehfard
JAJames Aluha
James Aluha
FGFrancois Gitzhofer
Francois Gitzhofer
Thermal spraying of aluminum nitride (AlN) is a challenging issue because it decomposes at a high temperature. In this work, the use of suspension plasma spray (SPS) technology is proposed for the in situ synthesis and deposition of cubic-structured AlN coatings on metallic substrates. The effects of the nitriding agent, the suspension liquid carrier, the substrate materials and the standoff distance during deposition by SPS were investigated. The plasma-synthesized coatings were analyzed by X-ray diffraction (XRD), optical microscopy (OM) and scanning electron microscopy (SEM). The results show higher AlN content in the coatings deposited on a carbon steel substrate (~82%) when compared to titanium substrate (~30%) or molybdenum (~15%). Melamine mixed with pure aluminum powder produced AlN-richer coatings of up to 82% when compared to urea mixed with the Al (~25% AlN). Hexadecane was a relatively better liquid carrier than the oxygen-rich liquid carriers such as ethanol or ethylene glycol. When the materials were exposed to a molten aluminum–magnesium alloy at 850 °C for 2 h, the corrosion resistance of the AlN-coated carbon steel substrate showed improved performance in comparison to the uncoated substrate.

16 September 2021 in Materials
Verified
Journal Article
Open access
PDF file
FGFrancois Gitzhofer
Francois Gitzhofer
JAJames Aluha
James Aluha
PLPierre-Olivier Langlois
Pierre-Olivier Langlois
FBFaranak Barandehfard
Faranak Barandehfard
TNThabang Abraham Ntho
Thabang Abraham Ntho
Nicolas AbatzoglouNicolas Abatzoglou
Nicolas Abatzoglou
The behavior of Mo in contact with molten Al was modelled by classical molecular dynamics (CMD) simulation of a pure Mo solid in contact with molten Al at 1200 K using the Materials Studio®. Results showed that no reaction or cross diffusion of atoms occurs at the Mo(s)–Al(l) interface, and that molten Al atoms exhibit an epitaxial alignment with the exposed solid Mo crystal morphology. Furthermore, the two phases {Mo(s) and Al(l)} are predicted to interact with weak van der Waals forces and give interfacial energy of about 203 mJ/m2. Surface energy measurements by the sessile drop experiment using the van Oss–Chaudhury–Good (VCG) theory established a Mo(s)–Al(l) interface energy equivalent to 54 mJ/m2, which supports the weak van der Waals interaction. The corrosion resistance of a high purity (99.97%) Mo block was then tested in a molten alloy of 5% Mg mixed in Al (Al-5 wt.%Mg) at 1123 K for 96 h, using the ALCAN’s standard “immersion” test, and the results are presented. No Mo was found to be dissolved in the molten Al-Mg alloy. However, a 20% mass loss in the Mo block was due to intergranular corrosion scissoring the Mo block in the ALCAN test, but not as a result of the reaction of pure Mo with the molten Al-Mg alloy. It was observed that the Al-Mg alloy did not stick to the Mo block.