As promising electrolyte materials in intermediate-temperature solid oxide fuel cells (IT-SOFCs), Sc-stabilized ZrO (ScSZ) and Y-stabilized ZrO (YSZ) electrolytes continue to be plagued by high cost and low intermediate conductivity. To mitigate these problems, Mn has been chosen as a new stabilization element for the synthesis of Mn-stabilized ZrO ceramics (MnSZ) through solid state sintering. Microstructures and electrical properties of micron-crystalline O (x = 0.15, 0.20 and 0.25) ceramics electrolytes for IT-SOFCs have been systematically evaluated. Within the applied doping content, Mn ions can enter the ZrO crystal lattice, leading to the formation of single cubic phase samples. Electrical conductivity measurements in the temperature range between 400 °C and 1000 °C show a sharp increase in conductivity due to Mn doping. The highest conductivity is obtained from the ZrMnO samples, being 0.0144 S/cm at 600 °C and 0.182 S/cm at 1000 °C. The electrical conductivity at 600 °C is twice higher than that of the YSZ and two orders of magnitude higher than that of the ScSZ. These properties can fulfill the conductivity requirement (∼1 S/cm) for the electrolyte. Therefore, based on this study, we propose that Mn stabilized ZrO is a promising candidate as a solid electrolyte for IT-SOFCs.
Anisotropic ZrO particles with octahedron-, diamond- and plate-like morphologies are successfully synthesized by a facile hydrothermal treatment approach using NaBF as mineralizer. The concentration of mineralizers play a crucial role on the formation of shape-controlled ZrO particles thus affect the particle size. With the increasing concentration of mineralizer, the crystalline sizes of the primary single-crystal and the secondary particle size both increase. With the introduction of NaBF, F plays an essential role in tuning the crystallinity and size of primary ZrO nanorods along [001] direction. The synergistic effect of F and B result in different epitaxial growth rate. And the secondary particles mainly crystallize on the small primary nanoparticles through the oriented attachment mechanism. The as-prepared ZrO particles with different sizes and shapes exhibit different photocatalytic efficiency for the degradation of organic dyes. Under UV irradiation, the highest MB degradation rate of 88% was observed within 60 min for ZrO photocatalyst synthesized with 0.01 mol/L NaBF mineralizer.
X-ray diffraction showed that an La7.0Mg75.5Ni17.5 alloy prepared via inductive melting was composed of an La2Mg17 phase, an LaMg2Ni phase, and an Mg2Ni phase. After the first hydrogen absorption/desorption process, the phases of the alloy turned into an La–H phase, an Mg phase, and an Mg2Ni phase. The enthalpy and entropy derived from the van’t Hoff equation for hydriding were −42.30 kJ·mol−1 and −69.76 J·K−1·mol−1, respectively. The hydride formed in the absorption step was less stable than MgH2 (−74.50 kJ·mol−1 and −132.3 J·K−1·mol−1) and Mg2NiH4 (−64.50 kJ·mol−1 and −123.1 J·K−1·mol−1). Differential thermal analysis showed that the initial hydrogen desorption temperature of its hydride was 531 K. Compared to Mg and Mg2Ni, La7.0Mg75.5Ni17.5 is a promising hydrogen storage material that demonstrates fast adsorption/desorption kinetics as a result of the formation of an La–H compound and the synergetic effect of multiphase.