Hui Peng

Prof. Hui Peng


Research Focus & Metrics

Academic Career Length

12Years (2015-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
15 April 2023 in Polymers
Verified
Journal Article
Open access
PDF file
YLYigang Lv
Yigang Lv
CWcui wang
cui wang
WHWeiwei Han
Weiwei Han
XLXing Li
Xing Li
Hui PengHui Peng
Hui Peng
Composites that use fly ash and slag as alkali-activated materials instead of cement can overcome the defects and negative effects of alkali-activated cementitious materials prepared with the use of an alkali-activated material. In this study, fly ash and slag were used as raw materials to prepare alkali-activated composite cementitious materials. Experimental studies were carried out on the effects of the slag content, activator concentration and curing age on the compressive strength of the composite cementitious materials. The microstructure was characterized using hydration heat, X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), mercury intrusion porosimetry (MIP) and scanning electron microscopy (SEM), and its intrinsic influence mechanism was revealed. The results show that increasing the curing age improves the degree of polymerization reaction and the composite reaches 77~86% of its 7-day compressive strength after 3 days. Except for the composites with 10% and 30% slag content, which reach 33% and 64%, respectively, of their 28-day compressive strength at 7 days, the remaining composites reach more than 95%. This result indicates that the alkali-activated fly ash–slag composite cementitious material has a rapid hydration reaction in the early stage and a slow hydration reaction in the later stage. The amount of slag is the main influencing factor of the compressive strength of alkali-activated cementitious materials. The compressive strength shows a trend of continuous increase when increasing slag content from 10% to 90%, and the maximum compressive strength reaches 80.26 MPa. The increase in the slag content introduces more Ca2+ into the system, which increases the hydration reaction rate, promotes the formation of more hydration products, refines the pore size distribution of the structure, reduces the porosity, and forms a denser microstructure. Therefore, it improves the mechanical properties of the cementitious material. The compressive strength shows a trend of first increasing and then decreasing when the activator concentration increases from 0.20 to 0.40, and the maximum compressive strength is 61.68 MPa (obtained at 0.30). The increase in the activator concentration improves the alkaline environment of the solution, optimizes the level of the hydration reaction, promotes the formation of more hydration products, and makes the microstructure denser. However, an activator concentration that is too large or too small hinders the hydration reaction and affects the strength development of the cementitious material.

25 February 2023 in Materials
Verified
Journal Article
Open access
PDF file
WHWeiwei Han
Weiwei Han
YLYigang Lv
Yigang Lv
SWShiyu Wang
Shiyu Wang
JQJie Qiao
Jie Qiao
CZchao chaosheng zou
chao chaosheng zou
Hui PengHui Peng
Hui Peng
The pH values of pore solutions are of great significance for the durability of concrete, but the influencing factors and mechanisms of geopolymer pore solutions are still unclear and the composition of raw material elements has a great influence on the geological polymerization behavior of geopolymers. Therefore, we prepared geopolymers with different Al/Na and Si/Na molar ratios using metakaolin, and the pH and compressive strength values of the pore solutions were determined using solid–liquid extraction. Finally, the influencing mechanisms of sodium silica on the alkalinity and geological polymerization behavior of geopolymer pore solutions were also analyzed. The results showed that the pH values of the pore solutions decreased with an increase in the Al/Na ratio and increased with an increase in the Si/Na ratio. The compressive strength of the geopolymers first increased and then decreased with an increase in the Al/Na ratio and decreased with an increase in the Si/Na ratio. The exothermic rates of the geopolymers first increased and then slowed down with an increase in the Al/Na ratio, indicating that the reaction levels first increased and then decreased with an increase in the Al/Na ratio. The exothermic rates of the geopolymers gradually slowed down with an increase in the Si/Na ratio, indicating that an increase in the Si/Na ratio reduced the reaction levels. In addition, the results obtained from SEM, MIP, XRD and other test methods were consistent with the pH change laws of geopolymer pore solutions, i.e., the higher the reaction level, the denser the microstructure and the smaller the porosity, whereas the larger the pore size, the smaller the pH value of the pore solution.

5 February 2024 in Materials and Structures
Verified
Journal Article
Closed access
PDF file
Bai ZhangBai Zhang
Bai Zhang
HZHong Zhu
Hong Zhu
TXTeng Xiong
Teng Xiong
Hui PengHui Peng
Hui Peng

11 January 2024 in Materials
Verified
Journal Article
Open access
PDF file
CCChao Cui
Chao Cui
YDYingze Dang
Yingze Dang
CLChenguang Luo
Chenguang Luo
LWLan Wang
Lan Wang
Hui PengHui Peng
Hui Peng
In this study, the influence of the physicochemical properties and proportioning conditions of metakaolin on the mechanical properties of the synthesized metakaolin geopolymers was comprehensively evaluated, and the issue of the reaction control mechanism for the formation of mechanical properties during the synthesis of geopolymers was addressed. The reaction mechanism was analyzed by SEM and FTIR, and the kinetic analysis of the geopolymerization process was carried out using isothermal calorimetry combined with the Jander model. The test results show that the physicochemical properties of the metakaolin and the proportioning conditions together affect the mechanical properties of the geopolymer, with the correlation between the active aluminum content of the metakaolin and the strength of the geopolymer reaching over 0.87. The early stages of the geopolymerization reaction are all controlled by nucleation–growth mechanisms (N < 1), and the variability in control mechanisms is mainly found in the later stages of the geopolymerization reaction. The low reactivity and slow exothermic hydration of metakaolin are more inclined to the nucleation-growth mechanism responsible for the hydration process due to the large amount of encapsulation.

26 November 2022 in Materials
Verified
Journal Article
Open access
PDF file
QZQingyu Zhong
Qingyu Zhong
Xiang TianXiang Tian
Xiang Tian
GXGuolun Xie
Guolun Xie
XLXi Luo
Xi Luo
Hui PengHui Peng
Hui Peng
In this study, geopolymer pastes with 60% metakaolin (MK) and 40% ground granulated blast-furnace slag (GGBFS) were synthesized. To determine the influence of the alkaline activator concentration, modulus, and the liquid/solid (L/S) ratio on setting time and compressive strength, the geopolymerization process and microstructures of MK/GGBFS-blended geopolymer pastes were analyzed using isothermal calorimetry, X-ray diffraction, mercury intrusion porosimetry, and scanning electron microscopy. Acid dissolution was employed to measure reaction extent. The results showed that the initial setting time of the geopolymer pastes was between 68 and 226 min, and the initial setting and final setting time was apart about by 10 min. For the same variable, the total heat released was positively correlated to the reaction extent. Available silicate content increased the reaction rate and intensity at the initial stage, whereas the OH− concentration controlled the reaction extent in the long term. A limited reaction extent existed in the geopolymeric reaction even if the system contained sufficient alkali content and medium. An increase in the L/S ratio increased the reaction extent. The highest reaction extent of 86.3% was found in the study. Additionally, increasing the L/S ratio reduced the compressive strength by increasing the porosity.

13 March 2023 in Materials
Verified
Journal Article
Open access
PDF file
YLYigang Lv
Yigang Lv
JQJie Qiao
Jie Qiao
WHWeiwei Han
Weiwei Han
BPBei Pan
Bei Pan
XJXiafei Jin
Xiafei Jin
Hui PengHui Peng
Hui Peng
Compared with Portland cement, geopolymers have poor carbonization resistance, which will greatly limit the application their application. To improve the carbonization resistance of geopolymers, firstly, the carbonization behavior of the fly ash-metakaolin-based geopolymer was studied through accelerated carbonization tests. Secondly, different amounts of Ca(OH)2 were introduced into the composite system, and the modification effect of the carbonization resistance of the modified geopolymer was studied. Finally, the modification effect of Ca(OH)2 on the fly ash-metakaolin-based geopolymers was analyzed, and the modification mechanism was explored. It was found that adding Ca(OH)2 to the fly ash-metakaolin-based geopolymer could significantly improve its initial compressive strength, but its strength after carbonization remained basically unchanged; meanwhile, the compressive strength of the terpolymer after carbonization clearly decreased after adding Ca(OH)2. Compared with ordinary Portland cement, the carbonization rate of fly ash-metakaolin-based geopolymer is faster, and the addition of Ca(OH)2 can inhibit the development of its carbonization depth. With increased carbonization age, the alkalinity of the geopolymer decreased, and the addition of Ca(OH)2 inhibited the decrease in the alkalinity of the geopolymer. The addition of Ca(OH)2 improved the microstructure of the geopolymers, the pore structure became denser, and the pore size became smaller size after carbonization. The hydration products of fly ash-metakaolin-based geopolymer are mainly amorphous silicaluminate gel and C–S–H gel, and Ca(OH)2 forms in the hydration products of terpolymer with the incorporation of Ca(OH)2, which is conducive to improving the carbonization resistance. In summary, Ca(OH)2 can play a good role in modifying the carbonization resistance of fly ash-metakaolin-based geopolymers.