The effect of high-temperature deformation twinning on the work hardening behaviors of Fe-38Mn alloy during hot shear-compression deformation was investigated. The discovery of micro-shear bands and deformation twinning is significant for continuous work hardening, and this represents an important step toward gaining a complete understanding of the effect of deformation twinning on work hardening behaviors. Deformation twinning is widely acknowledged to accommodate plastic strain under cold deformation, even under severe plastic deformation. At present, the equivalent stress vs. strain curves for hot shear-compression deformation of Fe-38Mn alloy exhibit the characteristics of continuous work hardening. In addition, continuous work hardening is classified into five stages when considering high-temperature deformation twinning.
The effect of deformation twinning on microstructure refinement was investigated for Fe-38Mn alloy during friction stir processing. It was proved that the friction stir processing microstructure of Fe-38Mn alloy was gradient distribution. The stir zone contained both recrystallized grains and fine deformed grains with average grain size of about 15 μm, and the proportion of twin boundaries in the deformed grain zone was up to 35%. Moreover, the cyclic multidirectional shear induced micro-shear bands and sub-grains with high density dislocations, as well as plentiful deformation twins. The microstructure refinement of Fe-38Mn alloy during friction stir processing resulted from the dynamic recrystallization mechanism and twinning mechanism. In addition, the cyclic multidirectional shear deformation enhanced the deformation twinning effect, so that the microstructure refinement process was completed quickly and effectively. The above works indicate a dynamic mechanism of microstructure refinement in term of the deformation twinning during friction stir processing.
The effect of high-temperature deformation twinning on the work hardening behaviors of Fe-38Mn alloy during hot shear-compression deformation was investigated. The flow curves for hot shear-compression deformation of Fe-38Mn alloy exhibit the characteristics of continuous work hardening. The deformation was uniform shear-compression deformation with no significant strain localization, but the shear action gradually increased with the increase of strain rate. Benefited from such deformation characteristics, the dynamic microstructure evolution was pioneered by “bulged” mechanism and had geometric and sub-grain migration characteristics, which was continuous dynamic recrystallization in nature and accompanied by a large number of micro-shear bands and deformation twins. Particularly, the work hardening rate curve is classified into five stages considering the deformation twinning during hot shear-compression deformation.