31 October 2022 in Materials
Verified
Journal Article
Open access
PDF file
DXDuotian Xia
Duotian Xia
RCRuilin Chen
Ruilin Chen
DZDuo Zhang
Duo Zhang
JCJianjun Cheng
Jianjun Cheng
In this study, the effects of different fine aggregates on the properties of polyethylene fiber engineered cementitious composite (PE-ECC) were systematically investigated. The PE-ECCs were prepared with four fine aggregates, respectively. Furthermore, their flowability, compressive strength, and uniaxial tensile properties were studied experimentally and comparatively analyzed by microscopic techniques including X-ray diffraction (XRD), scanning electron microscope (SEM), energy-dispersive spectroscopy (EDS), and mercury intrusion porosimetry (MIP). The results showed that all the different types of fine aggregates exhibited little effect on the flowability of PE-ECC, but a greater effect on the compressive strength, uniaxial tensile strength, and ultimate tensile strain. PE-ECC prepared from untreated desert sand showed the best comprehensive performance, with compressive strength, uniaxial tensile strength, and ultimate tensile strain of 47.92 MPa, 6.26 MPa, and 3.638%, respectively. Moreover, it was found that the ultra-fine particles in the desert sand promoted the hydration reaction of cement and produced more C–S–H gels. The pore structures of ECC prepared with different aggregates exhibited obvious fractal characteristics, and the fractal dimension ranged from 2.8 to 2.9. The fractal dimension showed a strong correlation with parameters including ultimate tensile strain and pore structure, and the larger the fractal dimension, the smaller the ultimate tensile strain, porosity, and average pore size of ECC.

1 July 2024 in Materials
Verified
Journal Article
Open access
PDF file
YLYupeng Li
Yupeng Li
AMAkelamjiang Maimait
Akelamjiang Maimait
JCJianjun Cheng
Jianjun Cheng
YDYanfu Duan
Yanfu Duan
YCYuanqing Chen
Yuanqing Chen
HDHongguang Dong
Hongguang Dong
Geopolymers, as a novel cementitious material, exhibit typical brittle failure characteristics under stress. To mitigate this brittleness, fibers can be incorporated to enhance toughness. This study investigates the effects of varying polypropylene fiber (PPF) content and fiber length on the flowability, mechanical properties, and flexural toughness of coal gangue-based geopolymers. Microstructural changes and porosity variations within the Fiber-Reinforced Geopolymer Mortar(GMPF) matrix were observed using scanning electron microscope (SEM) and Low field NMR(LF-NMR) to elucidate the toughening mechanism of PPF-reinforced geopolymers. The introduction of fibers into the geopolymer matrix demonstrated an initial bridging effect in the viscous geopolymer slurry, with a 3.0 vol% fiber content reducing fluidity by 5.6%. Early mechanical properties of GMPF were enhanced with fiber addition; at 1.5 vol% fiber content and 15 mm length, the 3-day flexural and compressive strengths increased by 30.81% and 17.4%, respectively. Furthermore, polypropylene fibers significantly improved the matrix’s flexural toughness, which showed an increasing trend with higher fiber content. At a 3.0 vol% fiber content, the flexural toughness index increased by 198.35%. The data indicated that a fiber length of 12 mm yielded the best toughening effect, with an 84.03% increase in the flexural toughness index. SEM observations revealed a strong interfacial bond between fibers and the matrix, with noticeable damage on the fiber surface due to frictional forces, and fiber pull-out being the predominant failure mode. Porosity testing results indicated that fiber incorporation substantially improved the internal pore structure of the matrix, reducing the median pore diameter of mesopores and converting mesopores to micropores. Additionally, the number of harmless and less harmful pores increased by 23.01%, while the number of more harmful pores decreased by 30.43%.

25 September 2024 in Buildings
Verified
Journal Article
Open access
PDF file
AMAkelamjiang Maimait
Akelamjiang Maimait
YWYaqiang Wang
Yaqiang Wang
JCJianjun Cheng
Jianjun Cheng
YDYanfu Duan
Yanfu Duan
ZPZhouyang Pan
Zhouyang Pan
Developing green, low-carbon building materials has become a viable option for managing bulk industrial solid waste. This paper presents a kind of all solid waste cementitious material (SWCM), which is made entirely from six common industrial wastes, including carbide slag and silica fume, that demonstrate strong mechanical properties and effectively stabilize aeolian sand (AS). Initially, we investigated the mechanical strength of waste-based cementitious materials in various mix ratios, focusing on their ability to stabilize river sand (RS) and aeolian sand. The results show that it is necessary to use alkaline solid waste carbide slag to provide a suitable reaction environment to achieve the desired strength. In contrast, the low reactivity of coal gangue powder did not contribute effectively to the strength of the cementitious material. Further orthogonal experiments determined the impact of different waste dosages on the strength of stabilized AS. It was found that increasing the amounts of carbide slag, silica fume, and blast furnace slag powder improved strength, while increasing fly ash first increased and then decreased strength. In contrast, higher additions of desulfurization gypsum and coal gangue powder led to a continuous decrease in strength. The optimized mix is carbide slag—desulfurization gypsum—fly ash—silica fume—blast furnace slag powder in a ratio of 4:2:2:3:3. The experimental results using SWCM to stabilize AS indicated a proportional relationship between strength and SWCM content. When the content is ≥20%, it meets the strength requirements for road subbases. The primary hydration products of stabilized AS are C-(A)-S-H, AFt, and CaCO3. Increasing the SWCM content enhances the reaction degree of the materials, thereby improving mechanical strength. This study highlights the mechanical properties of cementitious materials made entirely from waste for stabilizing AS. It provides a reference for the large-scale utilization of industrial solid waste and practical applications in desert road construction.

21 July 2025 in Materials
Verified
Journal Article
Open access
PDF file
WWWei Wang
Wei Wang
DLdi li
di li
DXDuotian Xia
Duotian Xia
RCRuilin Chen
Ruilin Chen
JCJianjun Cheng
Jianjun Cheng
The role and performance of desert sand in alkali-activated mortar remain insufficiently understood. To address this knowledge gap, this study systematically investigates the fluidity, mechanical properties, and microscopic morphology of alkali-activated mortar with varying desert sand substitution rates (DSRR, 0–100%). The key findings reveal that a low DSRR (10–20%) enhances mortar fluidity and reduces drying shrinkage, though at the cost of reduced compressive strength. At 40% DSRR, the mortar exhibits elevated porosity (12.3%) and diminished compressive strength (63 MPa). Notably, complete substitution (100% DSRR) yields a well-structured matrix with optimized pore distribution, characterized by abundant gel micropores, and achieves a compressive strength of 76 MPa. These results demonstrate that desert sand can fully replace river sand in alkali-activated mortar formulations without compromising performance. Microstructural analysis confirms that desert sand actively participates in the alkali activation process. Specifically, the increased Ca2+ content facilitates the transformation of amorphous gels into crystalline phases. It also found that desert sand could make the fly ash more soluble, affecting the alkali activation reaction.