Surrounding rock deformation and consequent support failure are the most prominent issues in red-bed rock tunnel engineering and are mainly caused by the effects of unloading, rheology, and swelling. This study investigated the mechanical responses of two kinds of red-bed mudstone and sandstone under unloading conditions via laboratory observation. Volume dilation was observed on the rocks during unloading, and the dilatancy stress was linear with the initial confining pressure. However, the ratios of dilatancy stress to peak stress of the two rocks kept at a range from 0.8 to 0.9, regardless of confining pressures. Both the elastic strain energy and the dissipated energy evolved synchronously with the stress–strain curve and exhibited conspicuous confining pressure dependence. Special attention was paid to the evolution behavior of the dilatancy angle. The dilatancy angle changed linearly during unloading. When the confining pressure was 10 MPa, the dilatancy angle of mudstone decreased from 26.8° to 12.5° whereas the dilatancy angle of sandstone increased from 34.6° to 51.1°; when the confining pressure rose to 25 MPa, the dilatancy angle of mudstone and sandstone decreased from 45.8° to 17.4° and increased from 21.7° to 39.5°, respectively. To further understand the evolution of the dilatancy angle, we discussed the links between the variable dilatancy angle and the processes of rock deformation and energy dissipation.
The void compression stage causes porous cement mortar to present special mechanical properties. In order to study the compaction behavior and the damage evolution of the porous material, cement mortar specimens with an average porosity of 26.8% were created and cyclic uniaxial compression tests were carried out. The irreversible strain accumulated in the tests was obtained by cyclic loading and unloading. As the secant modulus of the porous cement mortar increases with stress in the pre-peak deformation stage, its damage variable is defined according to the accumulated irreversible strain instead of modulus degradation. The strain-based damage indicator fitted with the damage evolution law is characterized by linear accumulation at the beginning and has an acceleration rate of about 0.3 in the pre-peak deformation stage, and the damage value converges to 1 at failure. Based on the Weibull distribution, a constitutive damage model of porous cement mortar is improved by considering both the damage evolution during the plastic deformation stage and the mechanical behavior in the compaction stage. The theoretical envelope curves obtained by the constitutive model are in good agreement with the experimental envelope curves of cyclic uniaxial compression in the compaction and pre-peak stages, and the average absolute error is about 0.54 MPa in the entire pre-peak stage, so the proposed damage constitutive model can characterize the damage-induced mechanical properties of porous cement mortar in the compaction and pre-peak stages.
6 February 2026 in Rock Mechanics and Rock Engineering
Mode II fracture toughness is an important material parameter of rocks, but accurate measurement of this parameter is still a challenge in rock fracture mechanics. This study aims to modify the mode II fracture toughness of red sandstone measured through shear box testing by emphasizing the critical role of crack initiation angle. Experimental tests combining fracture trajectory scanning and digital image correlation reveal distinct fracture mechanisms of red sandstone under varying loading angles: tensile spalling dominates low angles, and shear fractures emerge at medium angles, while tensile fracture initiates from the rock bridge center at high angles. Although shear fracture initiates from the notch tip, its initiation angle deviates from the initial crack plane, invalidating traditional mode II fracture toughness determination methods. A modified Mohr–Coulomb criterion incorporating fracture angle and Mode I stress intensity factor is proposed to correct the significant errors of traditional methods, and this study establishes a refined framework for mode II fracture toughness determination under compression–shear conditions.