The metal powder injection molding process is completed by mixing a metal powder and a binder, performing an injection molding and degreasing process, and then performing a sintering process for high density. The disadvantage of metal powder injection molding is that defects occurring during the process affect mechanical properties, which are worse in mechanical properties than in products manufactured by cold-rolling. In this study, the mechanical properties and microstructure of stainless steel 316L manufactured by the metal powder injection molding process were analyzed. Mechanical properties such as density, tensile strength, and fatigue life were analyzed. The density was measured using Archimedes’ principle, and a relative density of 94.62% was achieved compared to the theoretical density. The tensile strength was approximately 539.42 MPa and the elongation to fracture was approximately 92%. The fatigue test was performed at 80% of maximum tensile strength and a stress ratio of R = 0.1. The fatigue life was found in 55% (297 MPa) of maximum tensile strength that achieved 106 cycles. The microstructure was observed through scanning electron microscope after etching, and as a result, the average grain size was 88.51 μm. Using electron backscatter diffraction, inverse pole figure map, image quality map, and kernel average misorientation map of the specimen were observed in three different areas which were undeformed, uniformly deformed, and deformed. Based on these results, it is expected that research is needed to apply the metal powder injection molding process to the manufacture of agricultural machinery parts with complex shapes.

21 December 2023 in Journal of Materials Research and Technology
Verified
Journal Article
Open access
DLDohoon Lee
Dohoon Lee
SPSangwoo Park
Sangwoo Park
CLChan-Hee Lee
Chan-Hee Lee
HHHyun-Uk Hong
Hyun-Uk Hong
JOJongyeong Oh
Jongyeong Oh
BLByoungsoo Lee
Byoungsoo Lee

11 November 2022 in Materials & Design
Verified
Journal Article
Open access
CSChang-Seop Shin
Chang-Seop Shin
TDTruong Do
Truong Do
DLDohoon Lee
Dohoon Lee
TSTAE YEONG SO
TAE YEONG SO
SKSe-Hyun Ko
Se-Hyun Ko
PKPatrick Kwon
Patrick Kwon

10 September 2024 in Archives of Metallurgy and Materials
Verified
Journal Article
Closed access
DLDohoon Lee
Dohoon Lee
TSTAE YEONG SO
TAE YEONG SO
HYHa-Young Yu
Ha-Young Yu
GKGyunsub Kim
Gyunsub Kim
EMEushin Moon
Eushin Moon
SKSe-Hyun Ko
Se-Hyun Ko
A powder-bed-based additive manufacturing process called electron beam melting (EBM) is defined by high temperature gradients during solidification, which produces an extremely fine microstructure compared to the traditional cast material. However, porosity and segregation defects are still present on a smaller scale which may lead to a reduction in mechanical properties. It is important to have a better knowledge of the influence of post-fabrication treatments on the microstructure and mechanical characteristics before the use of additive manufacturing parts in specific applications. In this study, the effects of solution heat treatment (SHT) and hot isostatic pressing (HIP) on the microstructure and mechanical properties of Ti-6Al-4V alloy fabricated by the EBM process have been investigated. The SHT and HIP treatments can significantly improve the ductility of EBM Ti-6Al-4V due to the coarsening of α laths and the formation of β grains.

22 June 2026 in Archives of Metallurgy and Materials
Verified
Journal Article
Open access
PDF file
TSTAE YEONG SO
TAE YEONG SO
NAMSEOK KIMNAMSEOK KIM
NAMSEOK KIM
Shin Young-ChulShin Young-Chul
Shin Young-Chul
CCChang-Hee Cho
Chang-Hee Cho
In this study, the microstructural evolution of an A7075 aluminum alloy subjected to severe deformation by biaxial alternate forging (BAF) was investigated at room temperature (RT) and 300°C. SEM-BSE observations revealed no significant differences in the morphology or distribution of second-phase particles between the two conditions, indicating that deformation temperature did not markedly affect particle fragmentation at the applied strain level. However, SEM-EDS analysis of the matrix showed a noticeable reduction in Zn content after deformation at 300°C compared to RT, suggesting enhanced solute redistribution during high-temperature deformation. EBSD analyses demonstrated clear differences in deformation microstructures depending on both temperature and strain localization. At RT, the high-deformation region exhibited pronounced lattice distortion and heterogeneous orientation gradients, whereas deformation at 300°C resulted in more uniform IQ contrast and reduced intragranular misorientation, indicative of active recovery. Texture analysis based on ODF sections and pole figures showed moderate development of shear and rolling texture components, with more continuous and stabilized texture features at 300°C. These results indicate that elevated-temperature BAF promotes solute redistribution and recovery-assisted plastic flow without significant alteration of second-phase characteristics.