Space truss are widely used to cover large area.The main challenge of the composite space truss was transfer of shear from concrete slab to concrete. This paper presents an experimental study of the space truss with the concrete slab by introducing steel plates and bolts as shear connector. The Ultimate load carrying capacity of space truss 3 m × 2 m × 0.7 m with 50 mm concrete slab on the top was studied under two point loading. From the experimental results; it was observed that the composite action was achieved by introducing steel plate and bolts with the minimum slip of 0.82 mm and thereby strength and stiffness has increased. An analytical study using finite element analysis software ANSYS was carried out and it have subsequently compared with the experimental results.
This paper investigates the behaviour of axially-loaded tubular columns filled with M20 grade concrete and partially replaced concrete. The parameters varying in the study are slenderness ratio (13.27, 16.58 & 19.9), and normal M20 grade concrete, partially replaced quarry dust and concrete debris. The effects of the various concrete mixes and composite action between the steel tube and the concrete core are studied and a graph visualizing the differences between the load carrying capacity and the axial deflection is plotted. Some of the performance indices like the Ductility Index (DI), Concrete Contribution Ratio (CCR), Confinement Index (θ) and Strength Index (SI) are also evaluated and compared amongst the CFST columns. From the results it has been noted that an increase in the L/D ratio decrease the behaviour of the composite columns irrespective of the in filled materials. The composite action was achieved in the CFST columns filled with partially replaced quarry dust and concrete debris when compared with hollow steel columns. The load carrying capacity of the CFST column increases by 32 % compared with the hollow tubular columns.
24 September 2025 in Journal of King Saud University – Engineering Sciences
Materials undergo degradation and structural failure due to corrosion, leading to substantial economic losses in industrial applications. This study investigates the corrosion behavior and mechanical degradation of hot-rolled and cold-rolled mild steel in six different environments (air, tap water, seawater, NaCl, HCl, and H₂SO₄) over a period of 30 days. The analysis included weight loss, corrosion rate, thickness reduction, and mechanical strength evaluations at multiple intervals. Results revealed that cold-rolled specimens suffered up to a 55% loss in elongation and a 40% decline in tensile strength, particularly in acidic conditions. The superior performance of hot-rolled steel highlights the influence of manufacturing methods on corrosion resistance. Among all tested environments, sulfuric acid proved to be the most aggressive, with cold-rolled steel specimens exhibiting 10.212 mm and 5.649 mm of corrosion compared to 9.488 mm and 5.577 mm for hot-rolled steel specimens during the 30-day exposure period. Sulfuric acid exposure caused a maximum thickness reduction of 38.12%, along with a 40% loss in tensile strength and a 55% reduction in elongation at break for cold-rolled steel. Under the same exposure conditions, the compressive strength of hot-rolled specimens decreased by 25%. This comparative study offers valuable insights for designing durable steel structures and developing advanced corrosion mitigation strategies.
19 April 2021 in Arabian Journal for Science and Engineering