Piezoelectric materials (PEMs) find a wide spectrum of applications that include, but are not limited to, sensors, actuators, semiconductors, memory devices, and energy harvesting systems due to their outstanding electromechanical and polarization characteristics. Notably, these PEMs can be employed across several length scales (both intrinsic and extrinsic) ranging from mesoscale (bulk ceramics) to nanoscale (thin films) during their applications. Over the years, progress in probing individual electrical and mechanical properties of PEM has been notable. However, proportional review articles providing the mechanical characterization of PEM are relatively few. The present article aims to give a tutorial on the mechanical testing of PEMs, ranging from the conventional bulk deformation experiments to the most recent small-scale testing techniques from a materials science perspective. The advent of nanotechnology has led materials scientists to develop in situ testing techniques to probe the real-time electromechanical behavior of PEMs. Therefore, this article presents a systematic outlook on ex situ and in situ deformation experiments in mechanical and electromechanical environments, related mechanical behavior, and ferroelectric/elastic distortion during deformation. The first part provides significant insights into the multifunctionality of PEM and various contributing microstructural length scales, followed by a motivation to characterize the mechanical properties from the application's point of view. In the midst, the mechanical behavior of PEM and related mechanical characterization techniques (from mesoscale to nanoscale) are highlighted. The last part summarizes current challenges, future perspectives, and important observations.
The dry sliding wear behavior of as-cast pristine and boron-modified Ti-6Al-4V (Ti64) alloys (having 0.3 and 0.55 wt% B) is investigated using pin-on-disc experiments with the pin being Ti64 alloy and the EN31 steel disc. Experiments are performed at sliding speeds (s) of 1, 2, and 4 m/s and temperatures 300 and 573 K. A mixed response in wear behavior is observed. At the lowest sliding speed, all three alloys (except 0.55B alloy at 300 K) exhibit similar wear rates, with abrasive wear being the dominant wear mechanism. At 2 m/s, temperature and s increase, and adhesive wear takes over along with delamination wear. Here, the 0.55B sample shows the highest wear rate due to the debonding of more TiB particles, which increases three body abrasion wear. With further increase in s to 4 m/s, delamination and oxidation wear are observed for all the samples. XRD evaluation shows traces of TiO2 and Fe2O3, which imply the formation of MML in samples tested at s = 4 m/s, which is also validated through subsurface microstructure analysis. It is found that MML having more TiB particles has more stability, because of which 0.3B samples show higher wear rate.
1 August 2021 in Materials Science and Engineering: A