Engineered cementitious composites (ECCs) suffer from high shrinkage and low early strength due to large dosage of cementitious materials and slow hydration of fly ash. This study aims to improve compressive properties and reduce drying shrinkage of ECC using ceramic wastes and hydrothermal curing. Experimental results have indicated that ceramic polishing powder (CPP) and recycled ceramic sand (RCS) exert opposite effect on the compressive strength of ECC. Hydrothermal-cured ECC enhances elasticity modulus and compressive strength and reduces later drying shrinkage as compared with that under standard curing. A CPP dosage of 35% and a hydrothermal curing regime with a temperature of 70°C and age of 7 days are recommended for the engineering application of ECC.
Magnesium potassium phosphate cement (MKPC), made of sintered magnesium oxide and potassium phosphate, is a new material for construction and structural repair. It possesses high early strength and bond capacity, low drying shrinkage, excellent fire resistance and compatibility with concrete. These characteristics render it an ideal material for strengthening reinforced concrete (RC) structures. This study developed a MKPC-based textile reinforced cementitious composite (TRCC) to strengthen RC beams at soffit. Three-point flexural tests were conducted on two control specimens without strengthening and two strengthened specimens. Experimental results showed that the TRCC system exhibits good bonding with substrate concrete. The strengthened specimens failed due to rupture of textile meshes in TRCC. TRCC could improve load capacity by 4–25%, postpone propagation of cracks, reduce tensile strain of main reinforcement and reduce deflection of beams at the same load level. High relative textile ratios contributed to the load resistance while impaired the ductility of strengthened beams. Design formulae are proposed to predict the flexural capacity of beams strengthened by MKPC-based TRCC, and reasonable prediction close to experimental results can be obtained from the formulae.
1 April 2022 in Journal of Materials in Civil Engineering
This study investigated anchorage behavior of geopolymer-grouted rock bolts. Pull-out tests were conducted on rock bolts grouted by geopolymer mortar (GM), geopolymer paste (GP), and cement mortar (CM), respectively. The effect of grout, type of bolts, spacing of bolts, and anchorage depth on anchorage performance was examined. Experimental results have shown that GM achieves better bond than GP and CM under a constant water binder ratio of 0.4. Deformed bolts grouted by GM and GP exhibit a nominal bond strength 2.4 and 1.6 times higher than the plain round ones, respectively. Bolt spacing of more than 150 mm exerts little influence in the anchorage performance. Increasing anchorage depth contributes to both loading capacity and ductility, while reduces nominal bond strength of deformed bolts. The critical anchorage depth ensuring tensile failure of bolts is for both GM-grouted and GP-grouted bolts. GM-grouted deformed bolts with minimum anchorage depth of and bolt spacing of 150 mm are proposed for practical application.