Ion tracks formed in amorphous Ge by swift heavy-ion irradiation have been identified with experiment and modeling to yield unambiguous evidence of tracks in an amorphous semiconductor. Their underdense core and overdense shell result from quenched-in radially outward material flow. Following a solid-to-liquid phase transformation, the volume contraction necessary to accommodate the high-density molten phase produces voids, potentially the precursors to porosity, along the ion direction. Their bow-tie shape, reproduced by simulation, results from radially inward resolidification.
GexSi1−x alloy layers grown on (100) silicon substrates by molecular beam epitaxy and amorphized by ion irradiation at −196 °C are shown to recrystallize epitaxially during subsequent ion irradiation at 275 °C. This ion beam annealing process has been examined for two different sample configurations: the first consisting of a thin amorphous layer extending from the surface to about half the thickness of the alloy layer, and the second consisting of a thick amorphous layer extending beyond the alloy layer into the underlying silicon. In both cases, ion beam annealing results in epitaxial crystallization of the alloy layer. Results are reported for alloy composition in the range from Ge0.1Si0.9 to Ge0.8Si0.2.
Time‐resolved reflectivity and Rutherford backscattering spectrometry combined with channeling have been used to measure the epitaxial recrystallization kinetics of amorphous NiSi2 and CoSi2 layers. Epitaxial metal silicide layers, fabricated on (111) Si substrates by metal deposition and thermal reaction, were implanted with low‐energy Si ions to form amorphous surface layers. Such layers recrystallized epitaxially from the underlying crystalline metal silicide during thermal annealing at temperatures of 60–176 °C. Post‐anneal disorder consisted of dislocation networks as observed with transmission electron microscopy. Reduced recrystallization rates were apparent in samples implanted with O and Ar ions. Activation energies of 1.09±0.03 and 1.17±0.03 eV were determined for the epitaxial recrystallization of amorphous NiSi2 and CoSi2 layers, respectively.
A Pd-vacancy complex in Si has been identified with the perturbed angular correlation technique using the radioactive probe produced by recoil implantation. The fraction of Pd probes in the complex has been determined as a function of dopant type (B, P, As, and Sb), dopant concentration and annealing temperature . The complex, with a unique interaction frequency of , was observed only in with a maximum relative fraction of achieved between while a broad distribution of interaction frequencies was apparent in -, -, and . Annealing beyond yielded a reduction in the fraction with a dissociation energy of . Density functional theory calculations of the electric field gradient for the given defect configuration were consistent with a measured value of .
Ion beam induced epitaxial crystallization of amorphous NiSi2 is reported. Epitaxial NiSi2 layers on (111) Si substrates were implanted at ∼−196 °C with low‐energy Si ions to form an amorphous surface layer. The recrystallization of amorphous NiSi2 was induced at 13–58 °C by irradiating with high‐energy Si or Ne ions. Recrystallization proceeded in a layer‐by‐layer manner from the original amorphous/crystalline interface with an activation energy of 0.26±0.07 eV.