To control acid mine drainage (AMD) at source, biochar, a new green and environmentally friendly passivator has been introduced to passivate pyrite. However, the raw material and pyrolysis temperature largely determine the physical and chemical properties of biochar, the causal relationship between biochar and pyrite and the underlying mechanism are still unknown. Here, biochar materials (rice-straw biochar (RSB) and sugarcane bagasse biochar (SBB)) at different pyrolysis temperatures (300–600 °C) were utilized for the passivation of pyrite. The results of our investigations revealed that the passivation ability of RSB was superior to that of SBB. The addition of RSB with higher pyrolysis temperatures could greatly enhance the passivation efficiency of pyrite. RSB-500 (produced at a pyrolysis temperature of 500 °C) achieved the best passivation effect on pyrite. RSB can form Fe-O bonds through C=O bonding with pyrite. Moreover, the addition of RSB created a reducing environment in the mixture system because of its strong electron-donation capacity (EDC) and altered the energy-band structure of pyrite, which promoted the transfer of electrons from biochar to pyrite. On the contrary, the addition of SBB did not result in the formation of Fe-O bonds with pyrite. In addition, the EDC of SBB was also lower than that of RSB and it had almost no effect on the band structure of pyrite. Hence it did not alter the direction of the electron migration. These findings shed light on the mechanism of biochar passivation of pyrite and provide a theoretical foundation for selecting suitable biochar materials for AMD prevention at source.
Tailing ponds are major sources of heavy metal pollution. Previous studies primarily focused on tailings with high sulfur content, with limited attention to low-sulfur tailings. This study explored the release behavior of Pb, Zn, and Cd from low-sulfur tailings under simulated acid rain conditions, considering factors such as pH, particle size, and weathering degree. Samples were collected from a lead–zinc tailing pond in the karst regions of northern Guangxi, China. Batch leaching experiments indicated that even with high acid neutralization capacity (ANC = 166.57–167.45 kg H2SO4/t), substantial heavy metal leaching occurred under acidic conditions (pH 2–3), with Pb, Zn, and Cd concentrations increasing 4–6 times compared to neutral conditions. Leachate concentrations were slightly higher in coarser particles than in finer ones, while weathering further enhanced metal release, particularly for Cd. These findings suggest that acid neutralization alone may not be sufficient to prevent heavy metal leaching in low-sulfur tailings exposed to acid rain. However, due to the laboratory scale of this study, further validation through field-scale or mesocosm experiments is necessary to confirm the observed trends and assess their implications for environmental risk management in karst regions.