Cold-spray techniques have been a significant development for depositing metal coatings in recent years. In cold-spray processes, inexpensive nitrogen gas is widely used as the propellant gas in many industries. However, it is difficult to produce austenitic stainless steel coatings with dense microstructures with cold-spray techniques when using nitrogen propellant gas because of work hardening. In this study, the effects of cold-spray conditions using a nitrogen propellant gas on AISI 316L stainless steel coatings were examined. It was found that a higher nitrogen propellant gas temperature and pressure produce coatings with dense microstructures. The measured AISI 316L coating hardness values suggest that AISI 316L particles sprayed at temperatures of 700 and 800 °C soften due to the heat, allowing uniform deformation on the substrate and consequently forming dense coating microstructures. In addition, AISI 316L powder with particle diameters of 5–20 µm resulted in a denser coating microstructure than powder with particle diameters of 10–45 and 20–53 µm. Finally, the standoff distance between the nozzle and the substrate also affected the AISI 316L coating microstructures; a standoff distance of 40 mm produced the densest microstructure.
Cold-sprayed AISI 316L stainless steel coatings are treated to form an austenite phase with excessive dissolved nitrogen (known as the S-phase) by plasma nitriding at temperatures below 450 °C. The S-phase is a hard and wear-resistant layer with high corrosion resistance. However, the S-phase layer formed after only nitriding is thin and the hardness abruptly decreases at a certain depth; it lacks mechanical reliability. We examined two types of combined low-temperature plasma treatment to enhance the mechanical reliability of the S-phase layer: (i) sequential and (ii) simultaneous. In the sequential plasma treatment, the carburizing step was followed by nitriding. In the simultaneous treatment, the nitriding and carburizing steps were conducted at the same time. Both combined plasma treatments succeeded in thickening the S-phase layers and changed the hardness depth profiles to decrease smoothly. In addition, anodic polarization measurements indicated that sequential treatment involving carburizing followed by nitriding for 2 h each resulted in high corrosion resistance.