Tungstate and molybdate phosphors have received great attention for their excellent photoluminescent properties and thermal stabilities. In the article, Tb3+-activated tungstate and molybdate green phosphors were prepared by a solid-state reaction method at different caline temperatures and were compared and studied. The crystal structures and the morphologies of samples were characterized by X-ray diffraction (XRD) patterns and field emission scanning electron microscopy (FE-SEM) images. The energy-dispersive spectra (EDS) proved the compositions of the prepared samples. The photoluminescence (PL) spectra showed that the PL excitation spectra of Tb3+-doped Lu2W3O12 and Lu2Mo3O12 green phosphors consisted of a broad and strong charge transfer band (CTB) and 4f–5d transitions of Tb3+ in the ultraviolet (UV) wavelength range and some narrowed excitation peaks from the 4f–4f transition of Tb3+ in the near ultraviolet (NUV) wavelength region. The PL emission spectra of the phosphors exhibited the characteristic green emissions owing to the 5D4→7F5 transition of Tb3+ located at about 547 nm. The values of energy gap Eg were calculated based on the diffuse reflection spectra (DRS). The measuring temperature-dependent PL spectra illustrated the thermal stabilities of phosphors. The Tb3+-doped Lu2Mo3O12 phosphor presented normal thermal quenching phenomena and the values of the thermal activation energy Ea were calculated based on the measuring temperature dependent PL emission spectra. The Tb3+-doped Lu2W3O12 phosphor exhibited abnormal thermal enhancing CTB excitation intensity at about 170 °C. Furthermore, the PL decay curves suggested that the lifetime corresponding to the 5D4 level of Tb3+ in the Lu2W3O12 host lattice was longer than that in the Lu2Mo3O12 host lattice. Compared the Tb3+-doped Lu2Mo3O12 phosphor, the Tb3+-doped Lu2W3O12 phosphor has shown potential as an application in temperature sensors.
10 February 2022 in Journal of Physics: Condensed Matter
Two-dimensional (2D) van der Waals heterojunction offers alternative facile platforms for many optoelectronic devices due to no-dangling bonds and steep interface carrier gradient. Here, we demonstrate a 2D heterojunction device, which combines the benefits of high carrier mobility of 2D MoTe2 and strong light absorption of perovskite, to achieve excellent responsivity. This device architecture is constructed based on the charge carriers separation and transfer with the high-gain photogating effect at the interface of the heterojunction. The device exhibits high responsivity of 334.6 A W−1, impressive detectivity of 6.2 × 1010 Jones. All the results provide the insight into the benefits of interfacial carriers transfer for designing hybrid perovskite-2D materials based optoelectronic devices.
In this paper, Sm3+ doped Lu2W0.5Mo0.5O6, Lu2WMoO9, and Lu2(W0.5Mo0.5O4)3 materials were synthesized by using a two-step solid-state reaction method. The synthesized materials were characterized by X-ray diffraction (XRD) patterns, field emission scanning electronic micrograph (FE-SEM) pictures, photoluminescence (PL) excitation and emission spectra, and temperature-dependent emission intensities. Orange-reddish light could be observed from the phosphors under ultraviolet (UV) 365 nm light. The Sm3+ doped Lu2WMoO9 had enhanced PL intensities compared to the other two materials. The excitation, the energy transfer, the nonradiative relaxation, and the emission processes were illustrated by using schematic diagrams of Sm3+ in Lu2MoWO9. The optimal Sm3+ doping concentration was explored in the enhancing luminescence of Lu2WMoO9. By combing the Sm3+ doped Lu2WMoO9 to UV 365 nm chips, near white lighting emitting diode (W-LED) were obtained. The phosphor can be used in single phosphor-based UV W-LEDs.
Biomorphic Mn3O4 nanocrystal/porous carbon microfiber composites were hydrothermally fabricated and subsequently calcined using cotton as a biotemplate. The as-prepared material exhibited a specific capacitance of 140.8 F·g−1 at 0.25 A·g−1 and an excellent cycle stability with a capacitance retention of 90.34% after 5000 cycles at 1 A·g−1. These characteristics were attributed to the introduction of carbon fiber, the high specific surface area, and the optimized microstructure inherited from the biomaterial.