Cladding process can be used to create corrosion resistant surfaces from low cost materials. Austenitic stainless steel has been extensively used for weld cladding. It has excellent corrosion resistance and good weldability. In this context, experiments were conducted by depositing AWS E316LT1-1/4 stainless steel on to AISI 1020 carbon steel and the effects of flux cored arc welding (FCAW) process parameters on pitting and intergranular corrosion was investigated. Response surface methodology (RSM) based central composite design (CDD) was used to predict and develop the mathematical models for process parameters on corrosion resistance. The responses of interest were obtained by double loop electrochemical potentiokinetic reactivation (DLEPR) and potentiodynamic polarization tests. The process parameters analyzed were the wire feed rate, welding voltage, welding speed and nozzle to plate distance. All RSM models developed were statistically significant and presented good adjustments. The results indicated that the process parameters are important in determining the degree of sensitization and pitting potential, and the interaction between parameters cannot be neglected.
The present work investigates the effect of the initial microstructure on phase transformation after intercritical annealing by measuring the amount of austenite, which was obtained by X-ray diffraction and saturation magnetisation. Pieces of 8 Mn steel were austenitised at 1100°C for 1 h followed by different cooling rates: water, air, and furnace. Samples of each piece were subsequently intercritically annealed from 600 to 800°C followed by air cooling. The microstructure was characterised using scanning electron microscopy and electron backscatter diffraction. Results show how changing the cooling rate affects the temperature of intercritical annealing at which the highest content of retained austenite was obtained.
The effect of temperature on tensile and cyclic deformation is studied on SAE 1045 and SAE 4140 commercial steels. Tensile and low cycle fatigue (LCF) tests were performed at room temperature and 250°C. For a temperature of 250°C, an induction heating system was used during the tests. The temperature of the specimen was homogenized 600 s before testing. The tension-compression LCF tests were carried out at total strain amplitudes of ± 0.6%, ± 0.8%, and ± 1.0%. The Coffin-Manson-Basquim model was used to predict the LCF properties of steels. Scanning electron microscopy was used to evaluate the microstructure and the fracture surface. The fracture surfaces of samples tensile tested at room temperature and 250°C were similar. For fatigue testing, the surfaces obtained were also similar with regions of fatigue crack initiation and propagation, and rupture. A crack initiation near the surface was observed for the LCF specimens. Dynamic strain aging and recovery influenced the tensile and fatigue results, for example, the number of reversals to failure decreased for the fatigue test performed at 250°C. For fatigue tests performed at strain of 0.6% in the SAE 1045, the stress increased by 65% at 250°C when compared to testing at room temperature. Consequently, the number of reversals was reduced by 58%.