We report the dependence of the domain wall depinning field, domain wall velocity, including anisotropy direction, and magnetic properties on the oxidized aluminum thickness of perpendicularly magnetized asymmetric Pt/Co/AlOx trilayers. We also adopt the low-temperature magneto-transport measurement technique to investigate the amount of oxygen at the Co/AlOx interface of our magnetic thin films. At the lowest temperature of 25 K, it is found that the coercivity for the 5 nm aluminum thickness sample is very close to the average value and coercivity diminished above and below this critical aluminum thickness, hinting at a large variation in CoOx content at the interface. This tendency is also consistent with the modification of the depinning fields, coercive fields, and surface roughness measured at room temperature. Our results highlight an efficient way of controlling the depinning fields and other magnetic characteristics, which is important for stabilizing and driving magnetic spin textures and applicable to energy-efficient next-generation spintronics devices.
The morphology, crystallinity, and photoconductive properties of gallium nitride films grown by pulsed chemical vapor deposition on p-type Si(100) with and without ammonia (NH3) pretreatment are investigated. Ammonia pretreatments were performed at 525 °C and 800 °C, which resulted in GaN film thicknesses of 80 and 140 nm, respectively. An amorphous film of GaN is obtained without pretreatment and a polycrystalline GaN film with pretreatment. X-ray photoelectron spectroscopy showed that the pretreatment results in a 1–2 nm bilayer consisting of SiNx and SiOxNy at the GaN/Si interface. Photoconductive measurements show the 525 °C pretreated GaN film has a responsivity of 72 mA W−1 and a rise time of 0.37 ms, whereas the GaN film with an 800 °C pretreatment has a responsivity of 246 mA W−1 and a rise time of 1.7 ms. Moreover, the photocurrent of the 525 °C pretreated device exhibits superlinear power dependence with a power coefficient of 1.74, whereas the 800 °C pretreated device exhibits sublinear power dependence with a power coefficient of 0.58. The superlinear power dependence of the photoresponse of the 525 °C pretreated film is attributed to the presence of fast and slow recombination centers.