The micellar behaviour of similar hydrophobic chain length conventional (cetyltrimethyl ammonium bromide, CTAB; cetyl pyridinium chloride, CPC; cetyldimethylbenzyl ammonium chloride, C16BCl) and gemini surfactant (16-2-16) in water and polar non-aqueous solvents has been investigated in the temperature range 288.15–318.15 K with the help of conductivity measurements. The method proposed by Carpena et al. has been used to analyse the conductivity–concentration to determine the micellization parameters using critical micelle concentration (CMC) and degree of counter-ion dissociation (α) of the micelle. It shows much better performance than the conventional methods and the effect of experimental errors on the evaluation of the micellization parameters has been shown to be minimal by using this procedure. It was observed that the micellization tendency of the surfactant decreases in the presence of solvents. Thermodynamic parameters were also evaluated from the temperature dependence of the CMC values.
SrFe12O19 samples were initially prepared using sol-gel auto-combustion method and calcined from 500 to 1100°C (for 6 h). XRD data established the phase formation temperature of SrM phase to be ≈1000°C. Thereafter, the effect of Zn2+-Zr4+ co-dopant on magnetic and structural properties of SrZnxZrxFe12-2xO19 (x = 0.00–1.00) samples calcined between 900–1100°C was investigated. XRD data shows that the cell volume increases (from 690.45Å3 (x = 0.00) to 705.72Å3 (x = 1.00)) while crystallite size decreases (from 123.9 nm (x = 0.00) to 62.3nm (x = 1.00)) calcined at 1000°C. The Rietveld refinement of XRD data confirms a) x = 0.00 sample to be phase pure and b) the presence of ZnFe2O4 (≈2.25) & SrZrO3 (≈2.93%) impurity phases in x = 1.00 sample, calcined at 1000°C. FESEM micrographs revealed that a) grain size decreases for x > 0.20 with `x’ at 900°C and b) increases from 122 nm at 900°C to 443 nm at 1100°C, for x = 0.00. Broadening of Raman bands reveals generation of strain in the lattice with enhancement of Zn2+-Zr4+ concentration. The magnetic studies reveal that the coercivity monotonically decreases (from 5358(x = 0.00) Oe to 690(x = 1.00) Oe at 1000°C) with enhancement of Zn2+-Zr4+ concentration. A maximum Ms value ≈ 70.89 emu/g was observed in x = 0.20 sample at 1100°C. Ms value also decreases for x > 0.20 at each calcination temperature.