In this paper, (Tb0.7Lu0.3)2O3 magneto-optical transparent ceramics with different ZrO2 doping levels (0~5 at%) were prepared by hydrogen sintering and sequential HIP technique using ZrO2 as a sintering aid. The effect of ZrO2 doping content on the microstructure and optical properties of (Tb0.7Lu0.3)2O3 ceramics was analyzed. We found that the optimal doping content of ZrO2 was 3 at%. The transmittance of 3 at% ZrO2-doped (Tb0.7Lu0.3)2O3 ceramics at the wavelength of 1064 nm was 74.84 %, and the Verdet constant was approximately 275.28 rad·T−1·m−1 at the wavelength of 650 nm.
Magneto-optical transparent ceramics exhibiting the Faraday effect provide new opportunities for optical isolator applications. In this study, magneto-optical transparent ceramics (Tb0.94-xLu0.06Hox)2O3 (x=0, 0.005, 0.01, 0.0125, and 0.015) were successfully fabricated by reducing atmosphere sintering and hot isostatic pressing (HIP) post-treatment. The effect of x on the microstructure, in-line transmittance, and magneto-optical properties was studied. The addition of Ho3+ was found to promote the densification of the ceramics, enhancing their transmittance, with the in-line transmittance of (Tb0.93Lu0.06Ho0.01)2O3 reaching 79.05% at 1064 nm. Importantly, the Verdet constant was influenced by the doping of Ho3+. The highest Verdet constant belonging to (Tb0.925Lu0.06Ho0.015)2O3 was approximately −404 rad·T−1·m−1, which was approximately 6% higher than the undoped specimen, and more than 3 times that of the terbium gallium garnet (TGG) crystal.