In this study, 7075 aluminum alloy welding wire with TiB2 nanoparticle reinforcement as an additive together with the variable polarity TIG welding arc as a heat source were applied to produce thin-walled deposited layer samples. Results indicated that the performance of the deposited structure of 7075 aluminum alloy with a TiB2 reinforcement phase was significantly improved compared to the deposited structure of ordinary 7075 aluminum alloy welding wire. Meanwhile, the precipitation of the TiB2 reinforcement phase was insufficient within the structure, and the enhancing effect could not be fully exerted. Moreover, the 7-series aluminum alloy contained a large amount of Zn and Mg elements inside. If the soluble crystalline phase was not fully dissolved, severe stress corrosion could be caused, which inevitably led to a decrease in the mechanical properties. To further improve the performance of the deposited layer, a T6 heat treatment process was performed at 470 °C for 2 h, followed by rapid cooling with distilled water and artificial aging at 120 °C for 24 h. After heat treatment, many second phases appeared in the microstructure of the deposited layer, and the tensile strength increased from (361.8 ± 4.8) MPa to (510.2 ± 5.4) MPa together with the elongation which increased from (9.5 ± 0.5) % to (10.2 ± 0.4) %. The fracture mode of the fracture was a ductile fracture along grain boundaries. The microhardness increased from (145 ± 5) HV to (190 ± 4) HV and exhibited good corrosion resistance in a 3.5% NaCl solution corrosion test.
TIG arc additive manufacturing experiments were performed utilizing TiB2 nanoparticle-reinforced toward to 7075 aluminum alloy welding wire, and the microstructure and mechanical properties corresponding to different locations of welding plate were investigated. At the top location of the deposited layer, the microstructure was characterized by fine dendrite induced by solidification, and equiaxed grain was predominant at the middle location. The grain size at the bottom location was obviously larger compared to the top and middle locations, and secondary-phase particles were homogeneously distributed at the grain boundary or inner grains. The mechanical properties at the top location of the deposited layer were most excellent compared to the middle and bottom locations, and the tensile properties and micro-hardness were decreased with the detected area varying from middle location to the bottom location. The excellent combination of fracture elongation and maximum of tensile strength corresponding to different locations on the deposited layer were determined to be 361.8 MPa with respect to the 7075 aluminum alloy welding wire, respectively, which was higher compared to the samples processed by general arc additive manufacturing process with tensile strength of (279.4 ± 5.3) MPa, indicating the TiB2 nano-sized particles possessed certain enhancing effects on the investigated 7075 aluminum alloy.
2 January 2024 in Metallurgical and Materials Transactions A
In this paper, in situ SiC-reinforced Al-Zn-Mg-Cu composites were fabricated by laser powder bed fusion (LPBF). The effects of SiC content on the microstructure, phase composition, microhardness, and wear resistance of as-printed composites were preliminarily investigated. Results show that the microstructure was regulated, the matrix grains were refined, and the tendency to orientation grain growth was suppressed. SiC particles reacted in situ with the Al matrix to produce Si, Al4C3, and Al4SiC4 phases. The microhardness and wear resistance of as-printed composites increased with SiC content due to the fine grain strengthening of the matrix and the second phase strengthening of precipitates and reinforcements.
13 May 2024 in Journal of Materials Engineering and Performance