The aim of this work was to evaluate the porosity, microstructure, hardness, and electrochemical behavior of AISI 316 steel layers deposited on an AISI 347 steel substrate using the LMD process. Depositions of two, four, and six layers with a 0.5 mm height for each layer were performed at a speed of 375 mm/min, a power of 250 W, a focal distance of 5 mm, and without overlapping laser tracks. The results showed epitaxial growth of the deposited layers in relation to the substrate and a predominantly austenitic microstructure with ferrite as the substrate. The deposited layers presented a dendritic microstructure with a mean porosity of 4.5%. The porosity decreased as the number of deposited layers increased, affecting the pitting corrosion resistance. The sample with six deposited layers showed greater pitting corrosion resistance, whereas the corrosion current speeds were similar for the studied samples. Vickers hardness tests showed that the hardness decreased as the distance from the substrate increased, and the hardness decreased close to the remelted regions.
It was verified that SAE 4130 steel plates crack when laser beam welded at room temperature (RT). To overcome this problem, this work proposes a high temperature (HT) laser welding in order to reduce the residual stresses and create a bainitic structure instead of a martensitic one. A conventional post-welding heat treatment (PWHT) had been used as a comparison for HT. The centerline crack disappeared after a heat treatment of both in-situ (HT) or after inserting in a furnace (PWHT) at 500 °C for 10 minutes. The finite element analyses indicated a residual stress reduction from 163.70 to 3.72 MPa in the fusion zone (FZ) of the welds from RT to HT. The hardness obtained in FZ depends on the thermal cycle induced microstructure of the welds as 400 HV, 340 HV and 250 HV, for martensite (RT), tempered martensite (PWHT) and bainite (HT) micro-constituents. The proposed in-situ high-temperature laser beam welding method proved its usefulness to solve the center crack issue in SAE 4130 joints.
O objetivo deste trabalho é apresentar uma máquina para entalhamento de corpos de prova cerâmicos, bem como a escolha e a execução do entalhamento, usando SiC sinterizado via fase líquida, com adições de Al2O3 e Yb2O3, como material experimental para ser entalhado. Foi desenvolvido e construído, junto a uma empresa de S. Carlos-SP, um equipamento que permite produzir entalhes finos em corpos cerâmicos para posterior ruptura, visando determinar K IC pelo método SEVNB. Amostras de SiC com 10% de Al2O3+Yb2O3 foram sinterizadas a 1950 ºC, retificadas e entalhadas com lâminas de barbear e pastas diamantadas de 15, 9, 6, 3, 1 e 0,25 µm. A máquina produzida para o entalhamento das amostras está em operação no DEMAR-EEL-USP e, ao que se sabe, é a primeira no Brasil. Os resultados mostraram que em função da espessura da lâmina e da granulometria do agente abrasivo, pode-se produzir entalhes com diferentes raios de curvatura de sua ponta e profundidades.