Various testing methods and techniques have been used to identify and quantify per- and polyfluoroalkyl substances (PFAS) in food packaging. A common indirect measurement of PFAS is total fluorine (TF) and total organic fluorine (TOF). These methods are critical in rapidly screening food packaging materials for the >9000 PFAS and are often globally used for regulatory limits. However, this destructive approach requires careful sample preparation, combustion, and the analysis of the solution by a fluoride-specific electrode. The method described herein is a cost-effective, rapid, quantitative, and externally validated initial screening of packaging materials for fluoro-chemistry. This study presents validated protocols for measuring TF and TOF in packaging substrates using oxygen combustion sample preparation coupled with fluoride ion-selective electrode (F-ISE); the materials and required equipment are provided, and the step-by-step procedure from sample preparation to the analysis are described, including critical steps to minimize contamination and interferences during sample preparation.
Hermetic bag storage is a growing innovative technology that can effectively mitigate insect activity in stored grain and preserve quality without pesticides. This study aimed to estimate the environmental and economic impacts of hermetic storage bags as the basis for the sustainable adoption of the technology. This study demonstrated an approach to estimate the environmental impact of using hermetic bags and their superior economic benefits for storing maize at the 1-ton scale over three years. The life cycle assessment (LCA) of six commercially available hermetic bags (AgroZ®, GrainPro, Storezo, ZeroFly®, Elite, and PICS™) from cradle to grave was evaluated and compared using the Sustainable Minds LCA software. The gas barrier liners were analyzed for structure and polymer composition using confocal microscopy and Raman spectroscopy. The results showed that bag manufacturing had the highest environmental impact contribution, with 84.6% to 90.8% of the total impacts (mPt). The carbon footprint contribution of the total service life delivered for one hermetic bag ranged from 1.1 to 1.7 kg CO2eq. The economic benefits of using hermetic bags were calculated and compared with traditional storage bag methods for one smallholder farmer using ten (10) hermetic bags storing 100 kg/bag (1 ton) of maize. The results found that using hermetic bags exhibited the highest profit of 1130 USD when used for nine months over three years, while storage loss was maintained at less than 1%.
Polypropylene (PP) is one of the most abundant plastics used due to its low price, moldability, temperature and chemical resistance, and outstanding mechanical properties. Consequently, waste from plastic materials is anticipated to rapidly increase with continually increasing demand. When addressing the global problem of solid waste generation, post-consumer recycled materials are encouraged for use in new consumer and industrial products. As a result, the demand is projected to grow in the next several years. In this study, material recovery facility (MRF)-recovered post-consumer PP was utilized to determine its suitability for extrusion blow molded bottle food packaging. PP was sorted and removed from mixed-polymer MRF-recovered bales, ground, trommel-washed, then washed following the Association of Plastics Recyclers’ protocols. The washed PCR-PP flake was pelletized then manually blended with virgin PP resin at 25%, 50%, 75, and 100% PCR-PP concentrations and fed into the extrusion blow molding (EBM) machine. The EBM bottles were then tested for physical performance and regulatory compliance (limits of TPCH: 100 μg/g). The results showed an increased crystallization temperature but no practical difference in crystallinity as a function of PCR-PP concentrations. Barrier properties (oxygen and water vapor) remained relatively constant except for 100% MRF-recovered PCR-PP, which was higher for both gas types. Stiffness significantly improved in bottles with PCR-PP (p-value < 0.05). In addition, a wider range of N/IAS was detected in PCR-PP due to plastic additives, food additives, and degradation byproducts. Lastly, targeted phthalates did not exceed the limits of TPCH, and trace levels of BPA were detected in the MRF PCR-PP. Furthermore, the study’s results provide critical information on the use of MRF recovered in food packaging applications without compromising performance integrity.