The paper discusses a method of chemical polishing of Ti6Al4V samples and presents the results of our study. The samples were produced by selective laser melting, which is an increasingly popular method of producing thin-walled, geometrically complex products. The document analyzes how polishing with solutions featuring a varying content of hydrofluoric and nitric acids affects the etching rate and alters the superficial roughness of the samples in both the longitudinal and the transverse directions. We have thus formulated the recommendations on the optimum composition and concentration of such acidic solutions for polishing Ti6Al4V products made by selective laser melting.
At present, the selection of optimal technological parameters for laser powder bed fusion (LPBF) is determined by the requirements of the fusion process. The main parameters that are commonly varied include laser power (P), scanning speed (v), hatch spacing (h), and layer thickness (t). The productivity of the LPBF process (the increment in the fused volume of the material) is equal to the product of the last three parameters, and the mechanical properties are largely determined by the volumetric fusion energy density, which is equal to the ratio of laser power to productivity. While ensuring maximum process productivity, it is possible to obtain acceptable quality characteristics—mechanical properties, surface roughness, etc.—for a certain range of LPBF technological parameters. In these cases, several quality characteristics act as constraints on the optimization process, and productivity and the key quality characteristics become components of the objective function. Therefore, this article proposes a formalized representation of the optimization problem for the LPBF process, including the derivation of the objective function with the constraint matrix, and provides a solution to the problem using the linear programming (LP) method. The advantages of the proposed method include the guaranteed convergence of the solution with an unlimited number of constraints; the disadvantage concerns the adequacy of the solution, which is limited by a relatively narrow range of parameter changes. The proposed method was tested in determining the optimal LPBF parameters for an HN58MBYu powder LP model that included 13 constraints and an objective function with two target parameters. The obtained results made it possible to increase the productivity by 15% relative to the basic technological parameters.
7 July 2022 in VESTNIK of Samara University. Aerospace and Mechanical Engineering
This article provides an overview of the latest developments in the field of hybrid additive manufacturing of metal parts. The concept and various kinds of additive manufacturing are discussed. Special attention is paid to hybridization of additive technologies and various processes of forming: die forging, deep drawing, and others. The background and significance of the technologies, as well as their applicability in production are presented. The combination of additive manufacturing with forming processes is carried out with a dual purpose: to expand the area of application of additive manufacturing and overcome its limitations associated with low productivity, metallurgical defects, surface roughness and lack of dimensional accuracy; new application of traditional forming processes.
Samples of Ni-based super alloy are received by the method of direct metal deposition. Annealing at temperature 1180°С during 4 h is provided. Measurements of hardness, optical metallography, X-ray analysis are carried out. It was found that direct metal deposition of samples from Ni-based super alloy EP648 lead to Ni solid solution of alloying elements with face-centered cubic structure having lattice period a = 7.11 Å, also structure of Ni2Cr, is slightly revealed by optical metallography. Annealing at temperature 1180°С during 4 h of the direct metal deposited samples of super alloy EP648 lead to hardness increasing from от 19 ± 4 HRC to 34 ± 0.3 HRС, the uniformity of values are observed. After annealing the face-centered cubic structure is revealed, high value of lattice period is saving; presence of the phase Ni2Cr and sedimentation of Ni3Cr2 are found. Residual tensile macro stresses are found.
This study presents the development and validation of an in situ monitoring method for the laser direct energy deposition (DED) process, utilizing an integrated optical camera (720 HD, 60 fps) to analyze melt pool imagery. The approach is grounded in an experimental framework employing Taguchi orthogonal arrays, which ensures a stable dataset by controlling process variability and enabling reliable extraction of relevant features. The monitoring system focuses on analyzing brightness distribution regions within the melt pool image, identified as specific clusters that reflect external process conditions. The method emphasizes precise segmentation of the melt pool area, combined with automatic detection and classification of cluster features associated with key process parameters—such as focus distance, the number of deposited layers, powder feed rate, and scanning speed. The main contribution of this work is demonstrating the effectiveness of using an optical camera for DED monitoring, based on an algorithm that processes a set of melt pool identification features through computer vision and machine learning techniques, including Random Forest and HistGradient Boosting, achieving classification accuracies exceeding 95%. By continuously tracking the evolution of these features within a closed-loop control system, the process can be maintained in a stable, defect-free state, effectively preventing the formation of common process defects.
Work is focused on study of workability changing of heat resistant nickel-based Ni-15Co-10Cr alloy produced by selective laser sintering from metal powder. Experimental research of HRC hardness changing was provided on plate samples 2х10х30 mm after sintering and typical heat treatment for this alloy. Heat treatment was: annealing at temperature of 1,000oС during 1.5 hours, and then at the temperature of 1,180oC for 2.5 h – 3 h. After that samples were treated in a furnace for 50 – 60 minutes at the temperature of 1,050oС. Then they were cooled-off to the temperature of 1,000oС during 50 – 60 minutes. After that they were further quenched at ambient temperature. After quenching the samples were subjected to ageing at the temperature of 850oC during 3, 6, 9, 12 and 15 hours. The bending and measurement of triangle height was proposed for work ability assessment of samples. Increased hardness was found with duration of ageing. Work ability grew up with duration of ageing but where was a gap of workability for 9 hours ageing. Calibration of sintered parts and samples are recommended to perform after quenching and ageing at 850oC no longer 6 hours.