Self-powered ultraviolet (UV) photodetectors (PDs) based on GaN have been of great importance in the application of UV communication, thanks to its wide direct bandgap and strong resistance to irradiation. However, current self-powered GaN-based heterojunction UV photodetectors could not meet the requirement of fast photoresponse. Herein, type-II pn heterojunction GaS/GaN-based self-powered PDs have been proposed with a naturally p-type doping GaS thin film grown on n-type GaN via chemical vapor deposition. The electronic and optical properties of GaS/GaN heterojunction were investigated via experiments and the density functional theory. Afterward, as-prepared GaS/GaN-based PDs reveal an excellent self-powered photosensitivity/detectivity of 6.26 mA W−1/8.29 × 109 Jones at 0 V at 365 nm, ultrafast response speed with a rise/fall time of 48/80 μs as well as an amazing rejection ratio (R365 nm/R500 nm) of 3.42 × 104, and a fine rectification ratio of 105.9. This work provides a feasible method to synthesize high-performance GaS/GaN heterojunctions and demonstrates their enormous potential in ultrafast response self-powered UV photodetection.
Biochemical sensors have important applications in biology, chemistry, and medicine. Nevertheless, many biochemical sensors are hampered by intricate techniques, cumbersome procedures, and the need for labeling. In the past two decades, it has been discovered that liquid crystals can be used to achieve the optical amplification of biological interactions. By modifying recognition molecules, a variety of label-free biochemical sensors can be created. Consequently, biochemical sensors based on the amplification of liquid crystals have become one of the most promising sensors. This paper describes in detail the optical sensing principle of liquid crystals, sensing devices, and optical detection technologies. Meanwhile, the latest research findings are elucidated. Finally, the challenges and future research directions are discussed.
In this work, metal halide perovskite quantum dots (QDs) with Formamidinium (FA) and Cs mixed cations were fabricated using a solution-processed method at room temperature. By controlling Cs doping ratios in a precursor, the optical properties of mixed-cation perovskite QDs were systematically studied. With the increase in Cs ion doping, the photoluminescence (PL) spectra of perovskite QDs were blueshifted, which was mainly due to the smaller radius of Cs ions than those of FA. Temperature-dependent PL spectra were conducted on mixed-cation perovskite QDs. As the temperature gradually increased from 4 K to 300 K, PL peaks were blue shifted, and full-width at half maximum (FWHM) was widened, which was directly related to lattice thermal expansion and the carrier-photon coupling effect under temperature variation. At the same time, excess Cs ion doping had a prominent influence on optical properties at low temperatures, which was mainly due to the introduction of detrimental defects in perovskite crystals. Therefore, it is particularly important to control doping concentration in the preparation of high-quality perovskite QDs and efficient photoelectric devices.
Laser ablation of semiconductor silicon has been extensively studied in the past few decades. In the ultrashort pulse domain, whether in the fs scale or ps scale, the pulse energy fluence threshold in the ablation of silicon is strongly dependent on the pulse width. However, in the ns pulse scale, the energy fluence threshold dependence on the pulse width is not well understood. This study elucidates the interaction energy dependency on pulse width in ns NIR laser ablation of silicon. The level of ablation or melting was determined by the pulse energy deposition rate, which was proportional to laser peak power. Shorter pulse widths with high peak power were likely to induce surface ablation, while longer pulse widths were likely to induce surface melting. The ablation threshold increased from 5.63 to 24.84 J/cm2 as the pulse width increased from 26 to 500 ns. The melting threshold increased from 3.33 to 5.76 J/cm2 as the pulse width increased from 26 to 200 ns, and then remained constant until 500 ns, the longest width investigated. Distinct from a shorter pulse width, a longer pulse width did not require a higher power level for inducing surface melting, as surface melting can be induced at a lower power with the longer heating time of a longer pulse width. The line width from surface melting was less than the focused spot size; the line appeared either as a continuous line at slow scanning speed or as isolated dots at high scanning speed. In contrast, the line width from ablation significantly exceeded the focused spot size.