In the present work, zinc oxide (ZnO) nanoparticles were synthesized by direct precipitation method in aqueous solution using zinc acetate dihydrate and sodium hydroxide as precursors. The molar ratio of Zn2+ to OH– was 1:2. The obtained precipitated compound was treated at different temperatures. The crystal phase and structural parameters of each prepared ZnO samples such as interplanar spacing, crystallite size, dislocation density, micro strain were determined by X-ray diffraction (XRD) analysis for different crystallographic planes. Other crystallite parameters such as lattice constants, unit cell volume, Zn–O bond length, crystallinity of synthesized ZnO samples also were calculated from the XRD data. The XRD patterns show the successfully synthetized ZnO phase with wurtzite hexagonal structure and average crystallite sizes of 24.6 nm, 25.6 nm and 28.1 nm for the samples that dried at room temperature without heat treatment (S1), dried at 60°C without calcination (S2), dried at 60°C and calcinated at 300°C in air atmosphere for 2 hours (S3) respectively. The calculated structural parameters of the synthesized ZnO nanoparticles are in good agreement with the standard reported data (JCPDS 36-1451). The effect of heat treatment on the structural parameters of synthesized ZnO nanoparticles was examined and it indicates that increasing the thermal decomposition temperature improves the quality of crystalline material. The XRD data show that the synthesized S3 sample was free of impurities and characterized by lattice constants a = 3.252 Å, c = 5.210 Å, unit cell volume V = 47.703 Å3, bond length Zn–O = 1.9789 Å and crystallinity 93%. The results are of practical value for simple synthesis of highly dispersed forms of ZnO and its possible application in textile finishing.
22 May 2019 in Eastern-European Journal of Enterprise Technologies
The process of pretreatment of wool fiber is the main factor, which determines the state of the raw material base of wool. The prime cost and the quality of the finished products depend on how and in what way wool scouring was performed. The traditional technologies of the wool pretreatment are expensive and inefficient; furthermore, the problem of extraction of wool grease from the used washing waters is not paid sufficient attention to. The solution to this problem is applying innovative technology of highenergy discrete processing. Based on the conducted experimental studies, we proposed the technology of twostage wool scouring by the method of highenergy discrete processing, which includes the following sequence of technological operations: mechanical scouring of wool, the highenergy discrete processing of wool for 3 minutes, washing of wool in the SAS solution with the concentration of 1,5 g/l, at the temperature of 45 °C, washing of wool in clean water, drying.It was determined that the application of highenergy discrete processing of wool fiber for 3 minutes at the stage of washing contributes to improvement of the qualitative characteristics and to the increase in the output of wool grease up to 96 % in comparison with the amount of grease extracted from the unprocessed fiber.
Novel spherically shaped organosilica materials with (propyl)ethylenediamine groups were obtained via a modified one-pot Stöber co-condensation method. The porosity of these materials was tuned with the controlled addition of three silica monomers acting as structuring agents (tetraethoxysilane and bridged silanes with ethylene and phenylene bridges). The morphologies and structures of the synthesized materials were studied by SEM, DRIFT spectroscopy, CHNS elemental analysis, low-temperature nitrogen adsorption–desorption, and electrokinetic potential measurements. Their sizes were in the range of 50 to 100 nm, depending on the amount of structuring silane used in the reaction. The degree of the particles’ agglomeration determined the mesoporosity of the samples. The content of the (propyl)ethylenediamine groups was directly related with the amount of functional silane used in the reaction. The zeta potential measurements indicated the presence of silanol groups in bissilane-based samples, which added new active centers on the surface and reduced the activity of the amino groups. The static sorption capacities (SSCs) of the obtained samples towards Cu(II), Ni(II), and Eu(III) ions depended on the porosity of the samples and the spatial arrangement of the ethylenediamine groups; therefore, the SSC values were not always higher for the samples with the largest number of groups. The highest SSC values achieved were 1.8 mmolCu(II)/g (for ethylene-bridged samples), 0.83 mmolNi(II)/g (for phenylene-bridged samples), and 0.55 mmolEu(III)/g (for tetraethoxysilane-based samples).
22 August 2017 in Eastern-European Journal of Enterprise Technologies
Modification of coarse wool fibre is a basic condition for improving quality of the manufactured woolen textile products while reducing their cost. Traditional methods of modification of wool are expensive, that is why the implementation of these methods into existing technological modes is not always economically justified. The obtained effect of modification is often associated with undesirable damage of protein structure of fiber. A solution to this problem is the application of electric discharge treatment, accompanied by the emergence of electric discharge non-linear bulk cavitation. It is shown that the influence of electrohydrolic shock and products of water cleavage on wool does not cause profound destruction of keratin, in contrast to enzymatic and plasmochemical methods of treatment. Based on the performed experimental studies, it was determined that during electric discharge treatment of coarse wool there occurs the compaction of fiber cuticles and a change in supramolecular structure of keratin. This fact predetermines a decrease in felting ability of wool fibre, an increase in sorption properties, as well as in resistance to hydrolysis and influence of oxidants and reductants. It was established that the application of electric discharge treatment as a method of coarse wool modification would contribute to a decrease in shrinking and improvement of optimized dyeing of woolen textile material. Thus, the proposed technology of wool improvement will make it possible to use less expensive raw materials for the production of textile materials for different purposes.
A nanosized bifunctional adsorbent with diamino and phenyl groups on its surface is synthesized through the functionalization of silica derived from quartz. The composition, morphology, and particle size of the functionalized silica are characterized using various physicochemical methods. The material demonstrates high sorption properties for La(III) and Ce(III), both found in Ni‐MH batteries, as well as Eu(III). The synthesized functionalized silica, with adsorbed lanthanides, is employed for sensor‐based detection of doxycycline in aqueous solutions. After sorbing lanthanides, the bifunctional adsorbent shows a linear response to doxycycline in the concentration range of 0.005–10.0 µm, with a detection limit of 0.15 µm L−1 and a quantification limit of 0.44 µm L−1. The increase in photoluminescence signal upon the addition of doxycycline is explained using Judd–Ofelt theory. Experimental W2 and W4 parameters of the Eu‐doped nanomatrix are determined to be 1.44 × 10−20 cm2 and 8.55 × 10−20 cm2, respectively, with these values increasing to 73.40 × 10−20 cm2 and 35.58 × 10−20 cm2 upon the addition of doxycycline. A significant increase in the radiative emission rate from 196 s−1 to 1977 s−1 is observed with doxycycline addition. It is demonstrated that the system containing the three lanthanides exhibits unique sensor properties, attributed to the co‐luminescence of the Eu(III) ion.