In this study, we examined the effect of charging current density on the hydrogen embrittlement (HE) of MEA and the associated HE mechanisms using electron backscattered diffraction (EBSD). Results show that MEA is susceptible to HE, but is stronger than as-rolled and 3D-printed Cantor alloy and stainless steel. The HE susceptibility of MEA decreases with increasing current density. Ductile fracture with transgranular dimples switches to intergranular brittle fracture with clear slip bands in the interior of grains. EBSD results uncovered that hydrogen facilitates localized slips and deformation twins. Hydrogen-enhanced localized plasticity and hydrogen decohesion are the possible HE mechanisms.

27 August 2024 in Metals
Verified
Journal Article
Open access
PDF file
RRResearcher Researcher
Researcher Researcher
SYShaohua Yan
Shaohua Yan
ZZZhu Zhongyin
Zhu Zhongyin
The welded joints of high/medium entropy alloys (H/MEAs) have shown sound mechanical properties, indicating high promise for the industrial application of this new type of metal alloy. However, these joints possess either relatively low strength or low ductility. In this paper, we used ultrasonic-assisted laser welding to weld CrCoNi MEA with the nitrogen as shielding gas. The results showed that the tensile strength of the joint at room and cryogenic temperature is 686 MPa and 1071 MPa, respectively. The elongation at room and cryogenic temperature is 26.8% and 27.7%, respectively. The combination of the strength and ductility in our joints exceeds that of other welded H/MEA joints. We attributed this excellent combination to the refined dendrite, the solution of nitrogen into the matrix, and the low stacking fault energy of the CrCoNi MEA. The findings in this paper not only provide a novel way to weld H/MEAs with high strength and ductility, also are useful for additively manufacturing the high-performance component of H/MEAs.

4 January 2023 in Metals
Verified
Journal Article
Open access
PDF file
WCWenjing Chen
Wenjing Chen
WLWei Lu
Wei Lu
Guoqing GouGuoqing Gou
Guoqing Gou
LDLiwen Dian
Liwen Dian
ZZZhu Zhongyin
Zhu Zhongyin
JJJin Junjun
Jin Junjun
A7N01P-T4 aluminum alloy plates for high-speed trains will experience a certain amount of fatigue damage under alternating loads. Three groups of samples, P0 (no fatigue damage), P1 (loading stress 30 MPa), and P2 (loading stress 70 MPa), were created, and corrosion fatigue crack growth (CFCG) tests were conducted in 3.5 wt.% NaC1 solution. The crack growth rate was found to increase after fatigue damage as the damage degree increased. In addition, the A7N01P-T4 aluminum alloy base metal exhibited obvious secondary cracks and crack bifurcations after fatigue damage. It is believed that fatigue damage causes stress concentration in the material, while a certain degree of stress corrosion cracking occurs during the CFCG growth process. This is because hydrogen (H) easily accumulates and diffuses along the grain boundary, which reduces the strength of the grain boundary, thereby becoming the preferred orientation for crack growth. This explains why the CFCG rate of the material is accelerated following fatigue damage to a certain extent.

10 January 2023 in Metals
Verified
Journal Article
Open access
PDF file
MGMocheng Guo
Mocheng Guo
Guoqing GouGuoqing Gou
Guoqing Gou
BCBing Chen
Bing Chen
FQFeifei Qiu
Feifei Qiu
ZZZhu Zhongyin
Zhu Zhongyin
SSSongling Sun
Songling Sun
The measurement and control of residual stresses are crucial to the structural safety of high-speed trains. The critical refraction longitudinal wave method is extensively employed for the residual stress measurement, and the correction of the influencing factors is the key to the detection accuracy. However, the existing methods mostly give purely mathematical expressions which are only applicable to their studied materials. Hence, this paper proposes the specific influence factor correction method to enhance the applicability and accuracy, and the 5083 aluminum alloy welded component is utilized for testing. Subsequently, the stress coefficient K and the compensation acoustic time under the influence of internal factors are obtained by employing the proposed method, combined with the simulation to determine the focused detection zone, the hole-drilling and X-ray methods are utilized for comparisons, and the results indicate that the test data have a good coincidence. Meanwhile, the detection errors of each zone before and after the correction are analyzed. Moreover, combined with the experimental verification, it is found that the penetration depth of a critical refraction longitudinal wave approaches its one wavelength; the corresponding study is conducted with this characteristic and concludes that in the weld zone, the longitudinal residual stresses are mainly concentrated on the surface of the measured material. Finally, the above results indicate that the proposed method can provide more accurate measurements for engineering applications.

15 July 2026 in Materials
Verified
Journal Article
Open access
PDF file
CLChao Luo
Chao Luo
JGJun Gao
Jun Gao
Guoqing GouGuoqing Gou
Guoqing Gou
坷蒋坷君 蒋
坷君 蒋
ZZZhu Zhongyin
Zhu Zhongyin
First-principles calculations based on density functional theory (DFT) were employed to investigate the binding energy, work function, electronic structure, and optical properties of carbon quantum dots (CQDs) and nitrogen-doped carbon quantum dots (NCQDs) loaded on the TiO2(101) surface. The results indicate that NCQDs exhibit stronger binding affinity to the TiO2(101) surface than CQDs. The charge transferred from CQDs to the TiO2(101) surface mainly originates from the carbon atoms located at the two ends along the a-axis of the CQDs. By contrast, the charge distribution between NCQDs and TiO2(101) is more uniform, with the Bader charges of the carbon atoms at the two ends along the a-axis in NCQDs being reduced to varying degrees compared to those in CQDs. Moreover, loading NCQDs is more favorable for the generation of photogenerated electron-hole pairs and electron transfer, whereas loading CQDs leads to the smallest band gap.