This study, it is aimed to determine the adhesion strength of varnish layers applied to the surface of fresh and naturally aged wood materials. For this purpose, oak (Quercus Petrea L.), chestnut (Castanea sativa M.) and Scots pine (Pinus sylvestris L.) wood materials were used for each wood species, age period, section direction and varnish type. A total of 360 test samples were prepared and polyurethane, acrylic and water-based varnishes were applied to their surfaces. The adhesion strength of the samples was determined by the pull-off test following TS EN 4624. The statistical analyzes of the data obtained as a result of the experiments were made with the MSTAT-C package software, and the significance values between and within the groups were determined. According to the results of the research, it was determined that the age period did not affect the varnish adhesion strength the highest adhesion strength at the wood species level was obtained in chestnut (3.361 N/mm2), followed by oak (3.191 N/mm2) and Scots pine (2.248 N/mm2). At the varnish type level, the highest adhesion strength was obtained in polyurethane varnish (4.009 N/mm2), followed by acrylic varnish (3.754 N/mm2) and water-based varnish (1.286 N/mm2), respectively. In the section direction comparisons, the adhesion strength was found higher in the tangential direction (3.098 N/mm2) and higher in the radial direction (2.935 N/mm2). In the comparison level of age period-varnish type, the highest was obtained in polyurethane varnish (4.307 N/mm2) applied to the surface of naturally aged wood material, and the lowest was obtained in water-based varnish (1,167 N/mm2) applied to the surface of naturally aged wood material.
1 January 2009 in Procedia - Social and Behavioral Sciences
In this study, Computer Aided Design (CAD) education in the department of Furniture and Design, Technical Education Faculty, Gazi University, raises workforce for furniture industry and interior design sector, was investigated. A research questionnaire was developed and carried out with the students in accordance with the determination of problems, influence of education, teaching program and a comparative study of furniture design to classical drawing and CAD. As a result, the significant problem (96%) was found as the lack and insufficiency of CAD lectures in the teaching program. According to the study, CAD process is much more effective as the process as a whole is taken into consideration. It has been determined that new lectures are needed for the education of the visual presentation since 15hours is not sufficient. In reference to these results; there shall be a new approach to the CAD education of the department as a whole, where weekly lecture hours instead of diversity of the lectures shall be increased, since the process takes a long time; and the problems rising from lack of instructors shall be prioritised in the strategically planning
Bu çalışmada, doğal yaşlanmış ve yeni ağaç odunları üzerine uygulanan bazı verniklerin yüzey parlaklık değerleri (Gloss) araştırılmıştır. Her bir ağaç türü (3), kesit yönü (2), yaş periyodu (2) ve vernik çeşidi (3) deneme desenine göre 10’ar adet tekerrür olmak üzere toplam 360 adet deney örneği hazırlanmıştır. Doğal yaşlanmış ve yeni sarıçam (Pinus sylvestris L.), sapsız meşe (Quercus petrea L.) ve kestane (Castanea sativa M.) odunlarından hazırlanan deney örneklerine, ASTM-D 3023 standardı esaslarına göre, iki kat dolgu ve iki kat son kat vernik olmak üzere ipek mat su bazlı, ipek-mat poliüretan ve ipek-mat akrilik vernikler püskürtme tabancası ile uygulamıştır. Örneklerin yüzey parlaklıkları, TS EN ISO 2813 standardındaki esaslara uygun olarak belirlenmiştir. Deney sonuçlarına göre, yüzey parlaklığı yeni odunda (37,14) doğal yaşlanmış odundan (36,45) yüksek bulunmuştur. Ağaç türü düzeyinde, en yüksek sarıçamda (38,46) elde edilirken, sapsız meşe (35,89) ile kestane (36,04) arasındaki fark önemsiz çıkmıştır. Vernik çeşidi düzeyinde en yüksek parlaklık değeri poliüretan vernikte (39,88) elde edilmiş, bunu sırasıyla akrilik vernik (37,20) ve su-bazlı vernik (33,32) takip etmiştir.
In this study, the modulus of elasticity and flexural strength properties of laminated wood elements reinforced with steel mesh with different mesh openings were determined. In accordance with the purpose of the study, three- and five-layer laminated elements were produced from scotch pine (Pinus sylvestris L.) wood material, which is widely used in the wood construction industry in Türkiye. The 50, 70, and 90 mesh steel used as the support layer was placed between each lamella and pressed with polyvinylacetate (PVAc-D4) and polyurethane (PUR-D4) adhesives. Afterward, the prepared test samples were kept for 3 weeks at 20 °C temperature and 65 ± 5% relative humidity for 3 weeks. The flexural strength and modulus of elasticity in flexural of the prepared test samples were determined according to the TS EN 408: 2010+A1 standard by the Zwick universal tester. Multiple analysis of variance (MANOVA) was carried out using MSTAT-C 1.2 software to determine the effect of the modulus of elasticity and flexural strength on the obtained flexural properties, the mesh opening of the support layer, and the adhesive type. When the differences within or between groups were significant with a margin of error of 0.05, achievement rankings were made using the Duncan test on the basis of the least significant difference. According to the results of the research, the highest bending strength (120.3 N/mm2) was obtained in three-layer samples reinforced with 50 mesh steel wire and bonded with Pol-D4 glue, and the highest modulus of elasticity (8969.3 N/mm2) was obtained in three-layer samples reinforced with 50 mesh steel wire and bonded with Pol-D4 glue. As a result, the reinforcement of the laminated wood material with steel wire had an increasing effect on the strength. Accordingly, the use of 50 mesh steel wire can be recommended to increase mechanical properties.
In this study, strength properties of wood material reinforced with carbon fiber fabric, steel wire mesh and bamboo veneer were determined. Polyvinylacetate (PVAc) and polyurethane (PUR) glues (D4)were used for the lamellas obtained from Scotch pine (Pinus sylvestris L.) and eastern beech (Fagus orientalis L.). Compressive strength according to TS EN 408+A1; dynamic bending (shock) strength according toTS ISO 13061-10 and shear strength according to ASTM D 3110 were determined on 3 and 5-layers samples. According to the results, the highest compressive strength (62.8 N/mm2) was found in 5-layerseastern beech samples reinforced with carbon fiber fabric and bonded with PUR glue. The highest dynamic bending strength value (110.8 kJ/m2) was found in 5-layerseastern beech samples reinforced with carbon fiber fabric and bonded with PUR glue and the highest shear strength value (12.3 N/mm2) in 3-layered eastern beech samples reinforced with steel wire mesh and bonded with PUR glue.