Loïc Coulomb

Mr. Loïc Coulomb

Institut Charles Gerhardt, Montpellier, Occitanie, France
orcid

Research Focus & Metrics

Academic Career Length

6Years (2021-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
26 October 2021 in Nanomaterials
Verified
Journal Article
Open access
PDF file
LALinda Abbassi
Linda Abbassi
DMDavid Mesguich
David Mesguich
David BerthebaudDavid Berthebaud
David Berthebaud
STSylvain Le Tonquesse
Sylvain Le Tonquesse
Bhuvanesh SrinivasanBhuvanesh Srinivasan
Bhuvanesh Srinivasan
MBMickael Beaudhuin
Mickael Beaudhuin
Nanostructured β-FeSi2 and β-Fe0.95Co0.05Si2 specimens with a relative density of up to 95% were synthesized by combining a top-down approach and spark plasma sintering. The thermoelectric properties of a 50 nm crystallite size β-FeSi2 sample were compared to those of an annealed one, and for the former a strong decrease in lattice thermal conductivity and an upshift of the maximum Seebeck’s coefficient were shown, resulting in an improvement of the figure of merit by a factor of 1.7 at 670 K. For β-Fe0.95Co0.05Si2, one observes that the figure of merit is increased by a factor of 1.2 at 723 K between long time annealed and nanostructured samples mainly due to an increase in the phonon scattering and an increase in the point defects. This results in both a decrease in the thermal conductivity to 3.95 W/mK at 330 K and an increase in the power factor to 0.63 mW/mK2 at 723 K.

25 August 2023 in Journal of Alloys and Compounds
Verified
Journal Article
Closed access
RGRana Ghannam
Rana Ghannam
AMAdrien Moll
Adrien Moll
DBDavid Bérardan
David Bérardan
LCLoïc Coulomb
Loïc Coulomb
AVAntonio Vieira-E-Silva
Antonio Vieira-E-Silva
MBMickael Beaudhuin
Mickael Beaudhuin

2 February 2023 in Crystals
Verified
Journal Article
Open access
PDF file
DADoaa Omar A. Ali
Doaa Omar A. Ali
MFMarco Fabbiani
Marco Fabbiani
LCLoïc Coulomb
Loïc Coulomb
SBSimon Bosc
Simon Bosc
BVBenjamin Villeroy
Benjamin Villeroy
RVRomain Viennois
Romain Viennois
We present a new reactive spark plasma sintering (RSPS) technique for synthesizing the rhombohedral Ca14Si19 phase. The RSPS approach reduces the synthesis time from several weeks to a few minutes. The RSPS was found to be sufficient for obtaining a high level of purity of the Ca14Si19 under a pressure of 100 MPa for a dwell period of 5 min at a temperature of 900 ∘C. From electrical resistivity measurements, we were able to determine the energy band gap of Ca14Si19 to Eg=0.145(15) eV. The Seebeck coefficient shows Ca14Si19 as a p-type semiconductor at room temperature. It becomes n-type with increasing temperature pointing to significant bipolar and conduction band contributions due to the narrow bandgap of the compound.

29 December 2023 in Metals
Verified
Journal Article
Open access
PDF file
RVRomain Viennois
Romain Viennois
LALaurent Alvarez
Laurent Alvarez
LCLoïc Coulomb
Loïc Coulomb
YMYassine El Mastour
Yassine El Mastour
MFMarco Fabbiani
Marco Fabbiani
MBMickael Beaudhuin
Mickael Beaudhuin
We report on the successful synthesis of Bi1−xSbx alloys via mechanical alloying followed by sintering via spark plasma sintering, and the study of their lattice dynamics by Raman spectroscopy as well as their transport and thermoelectric properties. We observed an upshift of the frequency of the Raman-active Eg vibrational mode with increasing Sb content but no significant change for the frequency of the Raman-active A1g vibrational mode. Conversely, the linewidth of the Eg vibrational mode did not change significantly with increasing Sb content, whereas a twofold increase was observed for the A1g vibrational mode. Moreover, we confirm the emergence of several new vibrational modes with Sb alloying that could be associated with Bi-Sb and Sb-Sb vibrations. Rather large magnetoresistance was observed for all samples at room temperature. From the Seebeck coefficients, we determined the energy bandgaps in our samples, which are larger than those in bulk compounds, presumably due to the electronic confinement effect. We report a rather large thermoelectric power factor of 2–3 mW/m.K2 and thermoelectric figure of merit ZT of 0.15–0.23 at room temperature. However, ZT values were not improved at room temperature compared to prior works because of the rather large thermal conductivity of 3.75–4.5 W/m.K at room temperature. We find a larger resistivity, Seebeck coefficient, and power factor for the samples sintered at 200 °C for 5 min than for the samples sintered at 220 °C for 15 min, but similar thermal conductivity, resulting in larger ZT for the samples obtained in the first conditions. The samples with low Sb content x = 0.05 have a lower power factor and larger thermal conductivity than the samples with x = 0.12 and x = 0.15 for the same sintering conditions, which results in lower ZT for x = 0.05.