In order to seek for new Raman crystals, the manuscript presented the discussion on the Raman frequency of α-quartz, β-quartz, as well as Pb4+-doped SiO2 crystals at different temperature and pressure. The results demonstrated that as the pressure increased, the Raman lines shifted towards higher frequency for α-SiO2 crystal, while for β-SiO2 crystals, the main lines moved to lower frequency. Several new peaks were generated from the Pb4+-doped α-SiO2 crystals. The Pb4+-doped β-SiO2 crystals presented strong and ample Raman beams in the low-frequency range. The airfoil-shaped spectra appeared and broadened at high temperature and pressure. It could be inferred that the Pb4+-doped SiO2 crystals were excellent Raman crystal candidates.
In order to investigate the effect of the rare earth element Y on the strengthening potency of magnesium alloys and its strengthening mechanism under tension. In this paper, the solid solution structures with Y atom content of 1.8 at.% and 3.7 at.% were built, respectively, and their cohesive energies and stress-strain curve were calculated in the strain range of 0–20%. The calculation results of the cohesive energies showed that the structure of element Y is more stable with the increase of strains. The calculation results of stress and strain showed that Y element can improve the yield strength and tensile strength of the Mg-based alloy, and the strengthening effect is better when the Y content is 3.7 at.%.
In order to study the strengthening effect of Mg–X (X = Zn, Ag) alloys, solid solution structures of Mg54, Mg53X1 and Mg52X2 (X = Zn, Ag) with atomic contents of 1.8 at.% and 3.7 at.% were established, respectively. The structural stability, tensile properties and electronic properties were investigated by first-principles simulation. The calculated results of cohesive energies show that all solid solution structures were stable under different tensile strains, and Mg52Ag2 had the best stability. The results of tensile tests show that Zn and Ag atoms promoted the Mg-based alloy’s yield strength and tensile strength. In addition, through comparative analyses, we have demonstrated that the tensile property of Mg-based alloys was also affected by solid solubility. Finally, the electronic density of states (DOS) and electron density difference of several solid solution structures were analyzed.
Sapphire (α-Al₂O₃) is a leading optoelectronic and optical-window material whose transmission spans the deep-ultraviolet, visible and mid-infrared, covering the overwhelming majority of the useful optical spectrum. However, within this broad window the ultraviolet (UV) region is the most defect-sensitive region—the UV response of Ti:sapphire (Ti³⁺-doped α-Al₂O₃) is absorption-dominated, arising from interband transitions and the tail of the Ti 3d impurity bands. The microscopic defect origin of this UV response remains disputed, and how Ti³⁺-Ti³⁺ ion pairing reshapes the electronic and optical response has never been systematically studied. Here we present a first-principles density functional theory study that, for the first time, jointly maps the band structure, UV optical spectra (absorption, reflection and refraction), and temperature-/pressure-dependent Raman scattering of both single Ti³⁺-doped and Ti³⁺-Ti³⁺ ion-pair-doped α-Al₂O₃ in a 120-atom supercell. The results show that intrinsic Al₂O₃ is a wide-band gap insulator with a computed band gap of 7.065 eV, which is reduced to 4.722 eV upon single Ti³⁺ doping and to 3.480-4.588 eV for the three Ti³⁺-Ti³⁺ ion-pair configurations (line-, face- and point-contact). Doping introduces impurity levels near the Fermi level and gives rise to a new absorption peak in the 30-40 nm UV range, while the optical spectra shift systematically with doping concentration. Raman analysis shows that Ti³⁺ doping induces local lattice distortion and activates seven active vibrational modes (181-628 cm⁻¹); the characteristic peak areas grow with temperature, whereas the peak positions shift first to lower and then to higher wavenumbers with increasing pressure (reversing above 1.0 GPa). Together, these results unify how Ti³⁺ pairing governs the UV optical and vibrational response of sapphire, laying the groundwork for defect-engineered broadband optoelectronic materials.