Lingze Kong

Mr. Lingze Kong

orcid

Research Focus & Metrics

Academic Career Length

8Years (2019-Present)

(Calculated once Scilit publication data is synced: current year − year of first publication + 1)

Representative Publications

View All Publications
5 May 2021 in Propellants, Explosives, Pyrotechnics
Verified
Journal Article
Closed access
PDF file
LKLingze Kong
Lingze Kong
KDKehai Dong
Kehai Dong
YTYanhui Tang
Yanhui Tang
SLShuaiguang Lai
Shuaiguang Lai

1 July 2023 in Defence Technology
Verified
Journal Article
Open access
LKLingze Kong
Lingze Kong
KDKe-Hai Dong
Ke-Hai Dong
AJAi-Min Jiang
Ai-Min Jiang
CYChuan-Lu Yang
Chuan-Lu Yang
YTYan-Hui Tang
Yan-Hui Tang
YXYun-Dong Xiao
Yun-Dong Xiao

14 February 2023 in Molecules
Verified
Journal Article
Open access
PDF file
LKLingze Kong
Lingze Kong
KDKehai Dong
Kehai Dong
YTYanhui Tang
Yanhui Tang
CYChuan-Lu Yang
Chuan-Lu Yang
YXYundong Xiao
Yundong Xiao
Polyethylene glycols (PEG) and toluene diisocyanate (TDI) are often used as the main components of binders and curing agents in solid propellants, and their aging is an important issue in the storage and use of propellants. To study the aging behavior and aging mechanism of nitrate ester plasticized polyether propellant (NEPE) matrix during storage, the transition states of aging reactions of binder and curing agent were optimized at the (U)B3LYP/6-311G(d,p) level of theory, and the rate coefficients over the temperature range of 298–1000 K were calculated by CVT theory. The results showed that there were five kinds of aging reactions for binder, which included decomposition, nitration, H abstraction, oxidation, and crosslinking reactions. Among them, theenergy barriers of oxidation and H abstraction reactions were relatively low (79.3–91.2 kJ·mol−1) and the main reaction types of binder aging. The main aging reaction of curing agent was decomposition. Compared with the aging reactions of binder, the energy barriers of curing agent are higher (196.6–282.7 kJ·mol−1) and the reaction is more difficult to occur. By comparing the energy barriers and rate constants of different reactions, it is found that the aging of NEPE propellant matrix can be divided into two stages. In the first stage, the propellant matrix mainly undergoes H abstraction and oxidation reaction, and as the reaction proceeds, the products crosslink to form -O-O-, -C-C-, and -C-O-C- bonds. At this time, the long chain molecules of the propellant matrix crosslink, and the molecular weight increases. This stage corresponds to the rising stage of mechanical properties in the aging process of the propellant. In the second stage, the propellant matrix mainly undergoes decomposition and nitration, resulting in degradation, the reduction of molecular weights, and the appearance of holes and microcracks in the matrix. This stage corresponds to the decline of mechanical properties in the aging process of the propellant. The above simulation results are in good agreement with the aging experimental phenomena, revealing the microscopic mechanism of the changes in the macroscopic properties of NEPE propellant during the aging process, and providing a theoretical basis for the related research on the aging properties and anti-aging technology of NEPE propellant.

1 December 2019 in IOP Conference Series: Materials Science and Engineering
Verified
Conference Paper
Open access
PDF file
LKLingze Kong
Lingze Kong
KDKehai Dong
Kehai Dong
SCSitong Chen
Sitong Chen
CXCheng Xia
Cheng Xia
LPLiguan Pei
Liguan Pei
To obtain the aging mechanism of a certain kind of missile sealing nitrile rubber material under high and low-temperature cycle conditions, the nitrile rubber sealing ring was subjected to the accelerated aging test of high and low temperature circulating oil medium. The changes of compression set, mechanical properties, microstructure, molecular structure and dynamic mechanical properties under the condition of temperature-changing oil medium were studied. The dissociation energy of several important chemical bonds of nitrile rubber molecules was calculated. The test results show that the maximum tensile strength and elongation at break of special nitrile rubbers decrease with the increase of the number of cycles, and the compression set rate of nitrile rubber samples stored in oil medium increases gradually in the early stage of aging. Large, slightly restored in the late stage of aging, as the aging time increases, the side groups of the nitrile rubber molecules decompose and the main chain flexibility increases.

1 January 2024 in e-Polymers
Verified
Journal Article
Open access
PDF file
LKLingze Kong
Lingze Kong
WSWeiqi Sun
Weiqi Sun
HZHongqiang Zhao
Hongqiang Zhao
WZWei Zhou
Wei Zhou
FGFeng Guo
Feng Guo
RZRuiqi Zhong
Ruiqi Zhong
Polybutylene terephthalate (PBT) elastomers generated via the copolymerization of 3,3-bis(azidomethyl) oxetane and tetrahydrofuran have been widely used as a matrix for solid engines in rockets, missiles, and spacecraft because of their positive standard enthalpies of formation. This study investigates how the decomposition of PBT elastomers impacts their interactions with plasticizers during long-term storage and aging. We apply molecular dynamics to calculate the parameters (e.g., glass transition temperature, mechanical properties, diffusion, and compatibility) of PBT elastomers that influence the aging performance of PBT. The computational results indicate that as the degree of thermal-oxidative aging decomposition increases, the radius of gyration, peak value of radial distribution function, and free volume fraction of the aging model all decrease. The concomitant increase in defects and the weakening of the interactions between molecular chains in the aging model lead to a continuous reduction in the mechanical properties and glass transition temperature of the aging model. In general, the plasticizer exhibits enhanced diffusion and reduced compatibility. Overall, this article establishes models representing different degrees of thermal-oxidative aging of PBT elastomers, thereby revealing the interactions between plasticizers and PBT elastomers under thermal-oxidative aging conditions. The results provide a theoretical basis for evaluating the changes in the macroscopic aging performance of PBT elastomers from a microstructural perspective.