In the present study, the fatigue crack growth (FCG) behavior of short surface cracks in a fine-grained cemented carbide with a length of less than 1 mm was investigated. The rotating bending and the four-point bending fatigue tests were carried out at stress ratios of R = −1 and R = 0.1 (R = maximum stress/minimum stress). It was found that a short surface crack had a longer stable fatigue crack growth area than a long through-thickness crack; the FCG behaviors of the two types of crack are clearly different. Furthermore, the FCG path of short surface cracks was investigated in detail to study the interaction between fatigue cracks and microstructures of the cemented carbide such as WC grains and the Co phase. At a low Kmax (Kmax = the maximum stress intensity factor), it was found that fatigue crack growth within WC grains is difficult because of a small driving force; instead, crack growth is along the brittle WC/WC interface. On the other hand, at a high Kmax, WC grain breakage often occurs, since the driving force of FCG is large, and the fatigue crack grows linearly.
1 January 2014 in The Proceedings of the Materials and Mechanics Conference
In this study, the fatigue crack growth (FCG) characteristics of the short surface crack was studied at various stress ratios, R, using the fine grained cemented carbide. The FCG law for the material was studied using two parameters, the maximum stress intensity factor K max and the stress intensity factor range ΔK. It was found that the relationship between the rate of FCG, da/dN and ΔK depends on the R value. In the da/dN vs. K max relation, at the region of high crack growth rate, the FCG rate was nearly constant by the value of K max without depending on R. However, in the low FCG rate region, the FCG rate tended to accelerate as R became lower. Therefore, it was difficult to specify da/dN as a single value at different R ratios using either ΔK or K max from the low speed region to the high-speed region. For that reason, the FCG behaviour of the material was studied based on the crack growth law, da/dN = AK max mΔKn. The values of m and n were obtained as 6.6 and 1.4, respectively. Therefore, it was found that the FCG rate of the cemented carbide was strongly dependent on K max rather than ΔK, like the FCG characteristics of ceramics.