In blown powder additive manufacturing technologies the geometrical stability of the built parts is more complex with respect to more conventional powder bed processes. Because of this reason, in order to select the most suitable building parameters, it is important to investigate the shape and the properties of the single metal bead formation and the effect that a scan track has on the nearby ones. In the present study, a methodology to identify an appropriate laser metal deposition process window was introduced, and the effect of the building parameters on the geometry of circular steel samples was investigated. The effect of the scanning strategy on the deposited part was also investigated. This work draws the attention to the importance of the obtainment of the most suitable melt pool shape, demonstrating that the laser power and the scanning strategy have a strong influence not only on the shape but also on the mechanical properties of the final component.
In the last years, powder-based Laser Metal Deposition (LMD) has been attracting attention as a disruptive Additive Manufacturing (AM) technique for both the fabrication and restoration of Inconel 718 components, enabling to overcome current limitations faced by conventional manufacturing processes in terms of manufacturing costs, tool wear, and lead time. Nevertheless, the uncertainty related to the final mechanical performance of the as-built LMD parts limits a wider adoption of such technology at industrial level. This research work focuses on the mechanical characterization of as-built Inconel 718 specimens through split Hopkinson tensile bar tests performed at different strain rate conditions. The influence of laser power on the final mechanical behavior of the as-built tensile samples is discussed and compared with the mechanical response of as-cast ones. The as-built specimens exhibit a high internal density (i.e., 99.92% and 99.90% for 300 W and 400 W, respectively) and a more ductile behavior compared to the as-cast ones for every evaluated strain rate condition. The strain hardening capacity of the as-built samples increases with the laser power involved in the LMD process, reaching an average Yield Strength of 703 MPa for specimens realized at 400 W and tested at 800/s.
25 January 2021 in Metals and Materials International
Directed energy deposition is an additive manufacturing technology which usually relies on prototype machines or hybrid systems, assembled with parts from different producers. Because of this lack of standardization, the optimization of the process parameters is often a mandatory step in order to develop an efficient building process. Although, this preliminary phase is usually expensive both in terms of time and cost. The single scan approach allows to drastically reduce deposition time and material usage, as in fact only a stripe per parameters combination is deposited. These specimens can then be investigated, for example in terms of geometrical features (e.g. growth, width) and microstructure to assess the most suitable process window. In this work, Ti-6Al-4V single scans, produced by means of directed energy deposition, corresponding to a total of 50 different parameters combinations, were analyzed, focusing on several geometrical features and relative parameters correlations. Moreover, considering the susceptibility of the material to oxygen pick-up, the necessity of an additional shielding gas system was also evaluated, by comparing the specimens obtained with and without using a supplementary argon flow. A process window, which varies according to the user needs, was found together with a relationship between microstructure and process parameters, in both shielding scenarios.Graphic
In order to improve the process efficiency of a direct energy deposition (DED) system, closed loop control systems can be considered for monitoring the deposition and melting processes and adjusting the process parameters in real-time. In this paper, the monitoring of a new deposition nozzle solution for DED systems is approached through a simulation-experimental comparison. The shape of the powder flow at the exit of the nozzle outlet and the spread of the powder particles on the deposition plane are analyzed through 2D images of the powder flow obtained by monitoring the powder depositions with a high-speed camera. These experimental results are then compared with data obtained through a Computational Fluid Dynamics model. Preliminary tests are carried out by varying powder, carrier, and shielding mass flow, demonstrating that the last parameter has a significant influence on the powder distribution and powder flow geometry.