This study investigates the mechanical and durability performance of sustainable concrete using stone dust (SD) and ground sugarcane bagasse ash (GSCBA) to partially replace natural sand and cement, respectively. The experimental program was conducted with concrete containing 0–40 wt% GSCBA and 100% SD were prepared and tested. The results showed that full replacement of natural sand with SD did not significantly affect compressive strength. Concrete containing 10% GSCBA and 100% SD (10GSCBA) exhibited comparable compressive strength to the control concrete (CON) up to 90 days. However, the modulus of elasticity and modulus of rupture decreased slightly with increasing GSCBA content, indicating a close correlation with compressive strength. The mix containing 40% GSCBA and 100% SD (40GSCBA) achieved a compressive strength of 42.6 MPa at 90 days, representing 91% of the CON, with acceptable durability performance. These findings demonstrate that the combined utilization of SD and GSCBA offers an innovative and eco-efficient solution for concrete production, contributing to reduced cement consumption, lower production costs, and minimized carbon emissions without necessarily affecting mechanical strength or the long-term viability of the system.
This research investigates the development of an eco‐friendly geopolymer binder for pavement applications using fly ash mixed with waste materials, including bagasse ash and calcium carbide residue. These blended precursors were used as raw materials, activated with 5 M sodium hydroxide, a binder‐to‐solution ratio of 1:0.75 by weight, and a sodium hydroxide‐to‐sodium silicate ratio of 1:0.5. Compressive strength tests were conducted at 7 and 28 days under ambient curing. Microstructural characterization was performed using scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS), and x‐ray diffractometry (XRD), while the 3D pore and void structures were analyzed using x‐ray tomographic microscopy (XTM). The results revealed that the geopolymer contained high Si, Al, and Ca contents, making it suitable as a binder. The mix with 100% FA had the lowest pore volume and highest compressive strength. SEM and EDS mapping confirmed the formation of geopolymer gel, along with unreacted materials. Mixes with 85%–100% fly ash, and those with 40%–60% bagasse ash and calcium carbide residue, and 0%–20% fly ash, achieved compressive strengths of 30–40 MPa. The microstructural densification, indicated by reduced porosity observed through XTM, was identified as a key factor influencing the strength performance of the geopolymer binder. These findings suggest that optimized fly ash blended with waste materials (bagasse ash and calcium carbide residue) can produce a geopolymer binder with satisfactory strength, offering sustainable solutions for pavement applications.