This study experimentally analyzed the carbon dioxide adsorption capacity of Moso-bamboo- (Phyllostachys edulis-) based porous charcoal. The porous charcoal was prepared at various carbonization temperatures and ground into powders with 60, 100, and 170 meshes, respectively. In order to understand the adsorption characteristics of porous charcoal, its fundamental properties, namely, charcoal yield, ash content, pH value, Brunauer-Emmett-Teller (BET) surface area, iodine number, pore volume, and powder size, were analyzed. The results show that when the carbonization temperature was increased, the charcoal yield decreased and the pH value increased. Moreover, the bamboo carbonized at a temperature of 1000°C for 2 h had the highest iodine sorption value and BET surface area. In the experiments, charcoal powders prepared at various carbonization temperatures were used to adsorb 1.854% CO2for 120 h. The results show that the bamboo charcoal carbonized at 1000°C and ground with a 170 mesh had the best adsorption capacity, significantly decreasing the CO2concentration to 0.836%. At room temperature and atmospheric pressure, the Moso-bamboo-based porous charcoal exhibited much better CO2adsorption capacity compared to that of commercially available 350-mesh activated carbon.
8 March 2017 in The International Journal of Advanced Manufacturing Technology
This study presents the fabrication of high‐quality activated carbon (AC) from discarded coconut shells. The effects of experimental parameters such as activation temperature and activation time on the basic characteristics of AC, including charcoal yield, ash content, pH value, Brunauer‐Emmett‐Teller (BET) specific surface area, total pore volume, and iodine adsorption, are investigated. The results indicate that as the activation temperature and activation time increase, the charcoal yield of the AC decreases. In contrast, iodine adsorption, ash content, pH value, and total pore volume increase with activation temperature. The AC sample activated at 1000°C for 120 min had the highest BET specific surface area and total pore volume and thus the best CO 2 adsorption performance. This sample was compared with 30‐mesh commercial AC. The results reveal that coconut‐based AC has better instantaneous adsorption capabilities.
28 July 2015 in Physical Chemistry Chemical Physics
The separation of poisonous compounds from various process fluids has long been highly intractable, motivating the present study on the dynamic separation of H2S in acidic-gas-mixture-filled micropores. The molecular dynamics approach, coupled with the isothermal–isochoric ensemble, was used to model the molecular interactions and adsorption of H2S/CO2/CO/H2O mixtures inside metal-doped graphite slits. Due to the difference in the adsorption characteristics between the two distinct adsorbent materials, the metal dopant in the graphitic micropores leads to competitive adsorption, i.e. the Au and graphite walls compete to capture free adsorbates. The effects of competitive adsorption, coupled with changes in the gas temperature, concentration, constituent ratio and slit width on the constituent separation of mixtures were systematically studied. The molecule–wall binding energies calculated in this work (those of H2S, H2O and CO on Au walls and those of H2O, CO and CO2 on graphite walls) show good agreement with those obtained using density functional theory (DFT) and experimental results. The z-directional self-diffusivities (Dz) for adsorbates inside the slit ranged from 10−9 to 10−7 m2 s−1 as the temperature was increased from 10 to 500 K. The values are comparable with those for a typical microporous fluid (10−8–10−9 m2 s−1 in a condensed phase and 10−6–10−7 m2 s−1 in the gaseous state). The formation of H-bonding networks and hydrates of H2S is disadvantageous for the separation of mixtures. The results indicate that H2S can be efficiently separated from acidic gas mixtures onto the Au(111) surface by (i) reducing the mole fraction of H2S and H2O in the mixtures, (ii) raising the gas temperature to the high temperature limit (≥400 K), and (iii) lowering the slit width to below the threshold dimension (≤23.26 Å).