CuAgZr alloy is known for its high strength and high conductivity, which are reasons for its wide application. In this work, CuAgZr powder alloys were produced by high-pressure argon gas atomisation. The results indicate that the surface morphology of the powder is a cellular crystal structure with a pentagonal crystal structure, with a ‘rose-like’ lattice and cross-shaped dendrites. A three-dimensional model of the primary dendritic changes in the CuAgZr alloy powder with different powder diameters was established by studying the surface morphology and internal microstructure of the powder. The relationship between the powder diameter and the powder cooling rate was established as the function of the primary dendritic length (PDL), the primary dendritic volume fraction (PDVF), the secondary dendrite arm spacing (SDAS) and the secondary dendritic volume fraction (SDVF). A confidence validation was performed, and the function fitting error is within 10%. The results establish that the function is meaningful.
High-performance additives manufactured by Al alloys provide significant potential for lightweight applications and have attracted much attention nowadays. However, there is no research on Sc, Er and Zr microalloyed Al alloys, especially concerning corrosion behavior. Herein, crack-free and dense Al-Mg-Mn-Sc-Er-Zr alloys were processed by selective laser melting (SLM). After optimizing the process parameters of SLM, the anisotropic corrosion behavior of the sample (volume energy density of 127.95 J·mm−3) was investigated by intergranular corrosion (IGC) and electrochemical measurements. The results showed that the XY plane of the as-built sample is less prone to IGC, and it also has a higher open circuit potential value of −901.54 mV, a higher polarization resistance of 2.999 × 104 Ω·cm2, a lower corrosion current of 2.512 μA·cm−2 as well as passive film with superior corrosion resistance compared to the XZ plane. According to our findings, the XY plane has superior corrosion resistance compared to the XZ plane because it has fewer primary phases of Al3(Sc, Er, Zr) and Al2MgO4, which can induce localized corrosion. Additionally, a higher fraction of low-angle grain boundaries (LAGBs) and a stronger (001) texture index along the building direction are also associated with better corrosion resistance of the XY plane.
26 January 2023 in Transactions of the Indian Institute of Metals
The process of atomizing aluminum alloy powder using a rotating disk was studied by numerical simulation and experimental verification. The motion characteristics of the molten metal thin liquid film and the evolution law of atomization into droplets were systematically studied with different disk shapes and speeds. The results showed that the slippage of the liquid film on the surface of the spherical disk was smaller, the liquid film spread more evenly, and the velocity distribution was more uniform. Under the same working condition, the boundary diameter of the continuous liquid film on the spherical disk was 21–29% larger, and the maximum liquid film velocity increased by approximately 19%. In other words, the liquid film obtained more energy at the same rotational speed, the energy utilization rate was higher, and the liquid filaments produced by the splitting region of the disk surface were finer and greater in number. The data showed that the average thickness of the liquid film on the surfaces of different disk shapes was more affected by the speed of the flat disk, and the thickness on the spherical disk was relatively stable and uniform, but the difference in thickness between the two disk shapes decreased from 4.2 μm to 0.3 μm when the speed increased from 10,000 rpm to 60,000 rpm. In particular, the influence of the disk shape on the liquid film thickness became smaller when the speed increased to a certain range. At the same time, the characteristics of the liquid film during the spreading movement of molten metal on the disk and the mechanisms of the primary and secondary breakage of the liquid film were obtained through this simulation study.